Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Resist AG 100 - PMMA-I - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Resist AG 100:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Productprofil

PLEXIGLAS® Resist AG 100 is an amorphous thermoplastic molding compound, based on impact-modified polymethyl methacrylate (PMMA).

 

PLEXIGLAS® molding compounds have the following typical properties:

 

  • high weather resistance
  • excellent transmission and clarity
  • brilliant appearance
  • low weight – half the weight of glass
  • 100% recyclable – best life cycle assessment as compared with glass and PC
  • the pleasant feel and sound of the molded parts.

 

PLEXIGLAS® Resist AG 100 is characterized by the following special properties:

 

  • highest breaking strength and impact strength (30 times higher breaking strength than glass)
  • improved resistance to stress cracking
  • balanced property profile
  • clear reduction of reversible haze at very high and low temperatures
  • increased heat deflection temperature under load
  • AMECA listing, CAMPUS and moldflow data available

Application and approvals

PLEXIGLAS® Resist AG 100 has a balanced property profile and was specially developed for automotive glazing. This specialty molding compound meets all the relevant requirements for this field of application.
Apart from reducing the vehicle weight, injectionmolded glazing offers maximum freedom of design and functional integration, such as the integration of lighting or panel trim. An approval to ECE R43 is required for use as automotive glazing. The material has undergone and passed all tests in line with ECE R43.
The test report of the Materials Testing Agency in North Rhine-Westphalia is available for systems based on PLEXIGLAS® Resist AG 100 for rear side windows, roof and rear windows. Further details are available on request.

Processing

PLEXIGLAS® Resist AG 100 can be processed by injection molding of parts or by sheet extrusion and coextrusion. PLEXIGLAS® Resist AG 100 can be injection-molded on processing machines with a standard three-section screw for engineering thermoplastics in one-component or twocomponent processes.

Fabrication

Forming after extrusion
The forming conditions are the same as for extruded PLEXIGLAS®. The high optical quality of the surface after forming is also comparable. Predrying is not necessary in most cases. During heating, the material turns slightly white, but this disappears completely upon cooling.
Painting and screen printing
In principle, the same paints and lacquers can be used as for extruded PLEXIGLAS®. However, we recommend that you carry out preliminary tests in this case.
Coating
Surface coating, for example with polysiloxane systems, can be carried out by means of conventional processes.
Please send any questions on fabrication to automotive-glazing@evonik.com.

Physical Form / Packaging

PLEXIGLAS® Resist molding compounds are supplied as pellets of uniform size in 25kg polyethylene bags or 500kg boxes with PE lining. Other types of packaging are available on request.

Colors

PLEXIGLAS® Resist AG 100 for vehicle glazing is available in Clear-transparent (9V913). Beyond this, the transparent colors Green (6V176) and Gray (7V275) are available. Further colors on request: automotive-glazing@evonik.com

Sustainability

From production to recycling, the environmental impact of PLEXIGLAS® was tested in the life cycle assessment in accordance with ISO 14040ff and received a positive rating. In addition to its durability, PLEXIGLAS® offers convincing recyclability. It can be completely recycled by chemical conversion to its starting materials or directly reused.
Thus, in a study prepared by PE International AG, the environmental impacts during manufacture, application and disposal of automotive glazing made from PLEXIGLAS® were positively rated in comparison with reference systems (single-layer safety glass, laminated safety glass, PC). We will be pleased to provide more details on request.

加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 7.7 cm³/10min ISO 1133
温度 260 °C -
载荷 3.8 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2200 MPa ISO 527
屈服应力 55 MPa ISO 527
屈服伸长率 5 % ISO 527
名义断裂伸长率 45 % ISO 527
无缺口简支梁冲击强度, +23°C 120 kJ/m² ISO 179/1eU
热性能价值单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min 112 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 100 °C ISO 75-1/-2
热变形温度, 0.45 MPa 105 °C ISO 75-1/-2
维卡软化温度, B 105 °C ISO 306
线性热膨胀系数, 平行 110 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.6 mm -
Yellow Card 现存 是的 - -
光学特性价值单位Test Standard
ISO Data
光输送 91 % ISO 13468-1, -2
其它性能价值单位Test Standard
吸水性 1.5 % 类似ISO 62
吸湿性 0.5 % 类似ISO 62
密度 1160 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 250 °C ISO 294
注塑, 模具温度 82 °C ISO 294
注塑, 注射速度 195 mm/s ISO 294
函数
粘度-剪切速度 , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
剪切应力-剪切速度 , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
应力-应变(等时的) 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
蠕变模量-时间. 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
蠕变曲线 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
拉伸模量-温度 , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
典型数据
加工方法
注塑, 薄膜挤出成型, 异型材挤出成型, 片材挤出成型, 其它挤出成型, 热成型
供货形式
粒料
添加剂
脱模助剂
特殊性能
高冲击韧性的/经抗冲改性的, 经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 透明.
特征
无定形
耐化学试剂
耐环境应力裂纹性
应用
汽车
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
PREPROCESSING
预干燥温度: 70 - 80 ℃
在除湿型干燥器中的预干燥时间: 3-4h
PROCESSING
Température de la matière fondue: - °C
Température du moule: - °C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.