Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Resist AG 100 - PMMA-I - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Resist AG 100:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

Productprofil

PLEXIGLAS® Resist AG 100 is an amorphous thermoplastic molding compound, based on impact-modified polymethyl methacrylate (PMMA).

 

PLEXIGLAS® molding compounds have the following typical properties:

 

  • high weather resistance
  • excellent transmission and clarity
  • brilliant appearance
  • low weight – half the weight of glass
  • 100% recyclable – best life cycle assessment as compared with glass and PC
  • the pleasant feel and sound of the molded parts.

 

PLEXIGLAS® Resist AG 100 is characterized by the following special properties:

 

  • highest breaking strength and impact strength (30 times higher breaking strength than glass)
  • improved resistance to stress cracking
  • balanced property profile
  • clear reduction of reversible haze at very high and low temperatures
  • increased heat deflection temperature under load
  • AMECA listing, CAMPUS and moldflow data available

Application and approvals

PLEXIGLAS® Resist AG 100 has a balanced property profile and was specially developed for automotive glazing. This specialty molding compound meets all the relevant requirements for this field of application.
Apart from reducing the vehicle weight, injectionmolded glazing offers maximum freedom of design and functional integration, such as the integration of lighting or panel trim. An approval to ECE R43 is required for use as automotive glazing. The material has undergone and passed all tests in line with ECE R43.
The test report of the Materials Testing Agency in North Rhine-Westphalia is available for systems based on PLEXIGLAS® Resist AG 100 for rear side windows, roof and rear windows. Further details are available on request.

Processing

PLEXIGLAS® Resist AG 100 can be processed by injection molding of parts or by sheet extrusion and coextrusion. PLEXIGLAS® Resist AG 100 can be injection-molded on processing machines with a standard three-section screw for engineering thermoplastics in one-component or twocomponent processes.

Fabrication

Forming after extrusion
The forming conditions are the same as for extruded PLEXIGLAS®. The high optical quality of the surface after forming is also comparable. Predrying is not necessary in most cases. During heating, the material turns slightly white, but this disappears completely upon cooling.
Painting and screen printing
In principle, the same paints and lacquers can be used as for extruded PLEXIGLAS®. However, we recommend that you carry out preliminary tests in this case.
Coating
Surface coating, for example with polysiloxane systems, can be carried out by means of conventional processes.
Please send any questions on fabrication to automotive-glazing@evonik.com.

Physical Form / Packaging

PLEXIGLAS® Resist molding compounds are supplied as pellets of uniform size in 25kg polyethylene bags or 500kg boxes with PE lining. Other types of packaging are available on request.

Colors

PLEXIGLAS® Resist AG 100 for vehicle glazing is available in Clear-transparent (9V913). Beyond this, the transparent colors Green (6V176) and Gray (7V275) are available. Further colors on request: automotive-glazing@evonik.com

Sustainability

From production to recycling, the environmental impact of PLEXIGLAS® was tested in the life cycle assessment in accordance with ISO 14040ff and received a positive rating. In addition to its durability, PLEXIGLAS® offers convincing recyclability. It can be completely recycled by chemical conversion to its starting materials or directly reused.
Thus, in a study prepared by PE International AG, the environmental impacts during manufacture, application and disposal of automotive glazing made from PLEXIGLAS® were positively rated in comparison with reference systems (single-layer safety glass, laminated safety glass, PC). We will be pleased to provide more details on request.

Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 7.7 cm³/10min ISO 1133
Temperatura 260 °C -
Carga 3.8 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2200 MPa ISO 527
Tensão no escoamento 55 MPa ISO 527
Deformação no escoamento 5 % ISO 527
Deformação nominal na ruptura 45 % ISO 527
Resistência ao impacto Charpy , +23°C 120 kJ/m² ISO 179/1eU
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temp. de transição vítrea, 10°C/min 112 °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 100 °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 105 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 105 °C ISO 306
Coef. de expansão térmica linear, paralelo 110 E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB class IEC 60695-11-10
Espessuras do tubo de teste 1.6 mm -
Cartão Amarelo (yellow card) disponível sim - -
Propriedades ópticasValorUnidadeMétodo de ensaio
ISO Data
Transmitância luminosa 91 % ISO 13468-1, -2
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água 1.5 % Sim. to ISO 62
Absorção de umidade 0.5 % Sim. to ISO 62
Densidade 1160 kg/m³ ISO 1183
Produção de amostra para testeValorUnidadeMétodo de ensaio
ISO Dados
Moldagem por injeção, temperatura da massa 250 °C ISO 294
Moldagem por injeção, temperatura do molde 82 °C ISO 294
Moldagem por injeção, velocidade de injeção 195 mm/s ISO 294
Diagrama
Viscosidade - taxa de cisalhamento , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Tensão de cisalhamento - taxa de cisalhamento , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Tensão - deformação (isocrônico) 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Módulo de fluência - tempo 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Curva de fluencia 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Módulo de tração - temperatura , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Características
Processamento
Moldagem por injeção, Extrusão de laminas, Extrusão de perfis, Extrusão de chapas, Outros tipos de extrusão, Termoformagem
Forma de entrega
Granulos
Aditivos
Desmoldante
Características especiais
Alto impacto., Estável a luz, Estabilidade a raios U.V./Intempéries, Transparente
Características
Amorfo
Resistência Química
Resistência ao stress cracking
Aplicaciones
Automóvel
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Outras informações
Moldagem por injeção
PREPROCESSING
Predrying temperature: 70 - 80°C
Predrying time in a desiccant-type drier: 3 - 4 h
PROCESSING
Melt temperature: 235 - 270°C
Mold temperature:60 - 80°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.