Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Resist AG 100 - PMMA-I - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Resist AG 100:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Productprofil

PLEXIGLAS® Resist AG 100 is an amorphous thermoplastic molding compound, based on impact-modified polymethyl methacrylate (PMMA).

 

PLEXIGLAS® molding compounds have the following typical properties:

 

  • high weather resistance
  • excellent transmission and clarity
  • brilliant appearance
  • low weight – half the weight of glass
  • 100% recyclable – best life cycle assessment as compared with glass and PC
  • the pleasant feel and sound of the molded parts.

 

PLEXIGLAS® Resist AG 100 is characterized by the following special properties:

 

  • highest breaking strength and impact strength (30 times higher breaking strength than glass)
  • improved resistance to stress cracking
  • balanced property profile
  • clear reduction of reversible haze at very high and low temperatures
  • increased heat deflection temperature under load
  • AMECA listing, CAMPUS and moldflow data available

Application and approvals

PLEXIGLAS® Resist AG 100 has a balanced property profile and was specially developed for automotive glazing. This specialty molding compound meets all the relevant requirements for this field of application.
Apart from reducing the vehicle weight, injectionmolded glazing offers maximum freedom of design and functional integration, such as the integration of lighting or panel trim. An approval to ECE R43 is required for use as automotive glazing. The material has undergone and passed all tests in line with ECE R43.
The test report of the Materials Testing Agency in North Rhine-Westphalia is available for systems based on PLEXIGLAS® Resist AG 100 for rear side windows, roof and rear windows. Further details are available on request.

Processing

PLEXIGLAS® Resist AG 100 can be processed by injection molding of parts or by sheet extrusion and coextrusion. PLEXIGLAS® Resist AG 100 can be injection-molded on processing machines with a standard three-section screw for engineering thermoplastics in one-component or twocomponent processes.

Fabrication

Forming after extrusion
The forming conditions are the same as for extruded PLEXIGLAS®. The high optical quality of the surface after forming is also comparable. Predrying is not necessary in most cases. During heating, the material turns slightly white, but this disappears completely upon cooling.
Painting and screen printing
In principle, the same paints and lacquers can be used as for extruded PLEXIGLAS®. However, we recommend that you carry out preliminary tests in this case.
Coating
Surface coating, for example with polysiloxane systems, can be carried out by means of conventional processes.
Please send any questions on fabrication to automotive-glazing@evonik.com.

Physical Form / Packaging

PLEXIGLAS® Resist molding compounds are supplied as pellets of uniform size in 25kg polyethylene bags or 500kg boxes with PE lining. Other types of packaging are available on request.

Colors

PLEXIGLAS® Resist AG 100 for vehicle glazing is available in Clear-transparent (9V913). Beyond this, the transparent colors Green (6V176) and Gray (7V275) are available. Further colors on request: automotive-glazing@evonik.com

Sustainability

From production to recycling, the environmental impact of PLEXIGLAS® was tested in the life cycle assessment in accordance with ISO 14040ff and received a positive rating. In addition to its durability, PLEXIGLAS® offers convincing recyclability. It can be completely recycled by chemical conversion to its starting materials or directly reused.
Thus, in a study prepared by PE International AG, the environmental impacts during manufacture, application and disposal of automotive glazing made from PLEXIGLAS® were positively rated in comparison with reference systems (single-layer safety glass, laminated safety glass, PC). We will be pleased to provide more details on request.

Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 7.7 cm³/10min ISO 1133
Température 260 °C -
Charge 3.8 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2200 MPa ISO 527
Contrainte d'écoulement 55 MPa ISO 527
Déformation au seuil d'écoulement 5 % ISO 527
Déformation nominale à la rupture 45 % ISO 527
Résistance au choc Charpy, +23°C 120 kJ/m² ISO 179/1eU
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de transition vitreuse, 10°C/min 112 °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 100 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 105 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 105 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 110 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Yellow Card disponible oui - -
Propriétés optiquesValeurUnitéNorme du test
ISO Data
Transmittance 91 % ISO 13468-1, -2
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 1.5 % Sim. to ISO 62
Absorption d'humidité 0.5 % Sim. to ISO 62
Masse volumique 1160 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 250 °C ISO 294
Injection, température du moule 82 °C ISO 294
Injection, vitesse d'injection 195 mm/s ISO 294
Fonctions
Viscosité / Vitesse de cisaillement , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Contrainte de cisaillement / Vit. de cisaillement , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Contrainte / Déformation (isochrone) 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Module de fluage / Temps 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Courbe de fluage 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Module de traction / Température , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de profilés, Extrusion de plaques, Extrusion (autres), Thermoformage
Conditionnement
Granulés
Additifs
Agent de démoulage
Propriétés spéciales
Modifié choc, Stabilisé à la lumière, Stabilisé aux intempéries, Transparent
Caractéristiques
Amorphe
Résistance Chimique
Fissuration à l’environnement
Applications
Automobile
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Autres informations
Moulages par injection
PREPROCESSING
Predrying temperature: 70 - 80°C
Predrying time in a desiccant-type drier: 3 - 4 h
PROCESSING
Melt temperature: 235 - 270°C
Mold temperature:60 - 80°C
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.