Any use of this information falls under the rules of our
disclaimer.
Informations produit
MagicFil Thermo PLA is based on EasyFil PLA compound, but with a touch of thermochromic magic added, as MagicFil has a colour changing ability when heated above 29°C. MagicFil's anthracite grey colour will change into a natural PLA colour when the material reaches a temperature of 29°C or above.
Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test |
Other Standards[S] |
Indice de fluidité, MFI |
6 |
g/10min |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés mécaniques | Valeur | Unité | Norme du test |
Other Standards[S] |
Module de flexion |
2392 |
MPa |
|
Résistance à la flexion |
55.2 |
MPa |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés thermiques | Valeur | Unité | Norme du test |
ASTM Data |
Température de fusion |
210 |
°C |
ASTM D 3418 |
Propriétés optiques | Valeur | Unité | Norme du test |
ASTM Data |
Brillant |
90[1] |
- |
ASTM D 2457 |
Haze |
2.1 |
% |
ASTM D 1003 |
Propriétés diverses | Valeur | Unité | Norme du test |
Densité |
1240 |
kg/m³ |
ASTM D 792 |
Propriétés mécaniques (Grades film) | Valeur | Unité | Norme du test |
ASTM Data |
Module en traction, long. |
3310 |
MPa |
ASTM D 882 |
Module de traction, long. |
110 |
MPa |
ASTM D 882 |
Allongement à la rupture, long. |
160 |
% |
ASTM D 882 |
Caractéristiques
Transformation
Additive Manufacturing
Conditionnement
Monofilament
Propriétés spéciales
Modifié choc
Caractéristiques
Bonne adhérence
Certifications
Contient des ressources renouvelables
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com