MagicFil Thermo PLA is based on EasyFil PLA compound, but with a touch of thermochromic magic added, as MagicFil has a colour changing ability when heated above 29°C. MagicFil's anthracite grey colour will change into a natural PLA colour when the material reaches a temperature of 29°C or above.
Características de processamento/físicas | Valor | Unidade | Método de ensaio |
Other Standards[S] |
Índice de fluidez, MFI |
6 |
g/10min |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriedades mecânicas | Valor | Unidade | Método de ensaio |
Other Standards[S] |
Módulo de flexão |
2392 |
MPa |
|
Resistência à flexão |
55.2 |
MPa |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriedades térmicas | Valor | Unidade | Método de ensaio |
ASTM Dados |
Temperatura de fusão |
210 |
°C |
ASTM D 3418 |
Propriedades ópticas | Valor | Unidade | Método de ensaio |
ASTM Dados |
Brilho |
90[1] |
- |
ASTM D 2457 |
Haze |
2.1 |
% |
ASTM D 1003 |
Outras propriedades | Valor | Unidade | Método de ensaio |
Densidade |
1240 |
kg/m³ |
ASTM D 792 |
Propriedades do filme | Valor | Unidade | Método de ensaio |
ASTM Data |
Módulo de tração, long. |
3310 |
MPa |
ASTM D 882 |
Resistência à tração, long. |
110 |
MPa |
ASTM D 882 |
Deformação na ruptura, long. |
160 |
% |
ASTM D 882 |
Características
Processamento
Additive Manufacturing
Forma de entrega
Monofilament
Características especiais
Alto impacto.
Características
Boa adesão
Certifications
Contém recursos renováveis
Disponibilidade regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.