Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Makrolon® 2405 RE - PC - Covestro Deutschland AG
Material Data Center offers the following functions for Makrolon® 2405 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Informations produit
- MVR (300 °C/1.2 kg) 19 cm³/10 min
- general purpose
- low viscosity
- easy release
Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test |
ISO Data |
Indice de fluidité à chaud en volume, MVR |
19 |
cm³/10min |
ISO 1133 |
Température |
300 |
°C |
- |
Charge |
1.2 |
kg |
- |
Indice de fluidité, MFI |
20 |
g/10min |
ISO 1133 |
Température |
300 |
°C |
- |
Charge |
1.2 |
kg |
- |
Retrait au moulage, parallèle |
0.7 |
% |
ISO 294-4, 2577 |
Retrait au moulage, perpendiculaire |
0.7 |
% |
ISO 294-4, 2577 |
Propriétés mécaniques | Valeur | Unité | Norme du test |
ISO Data |
Module en traction |
2400 |
MPa |
ISO 527 |
Contrainte d'écoulement |
65 |
MPa |
ISO 527 |
Déformation au seuil d'écoulement |
6 |
% |
ISO 527 |
Déformation nominale à la rupture |
>50 |
% |
ISO 527 |
Module de flexion, 23°C |
2350 |
MPa |
ISO 178 |
Résistance à la flexion |
97 |
MPa |
ISO 178 |
Module de fluage en traction, 1h |
2200 |
MPa |
ISO 899-1 |
Module de fluage en traction, 1000h |
1900 |
MPa |
ISO 899-1 |
Résistance au choc Charpy, +23°C |
N |
kJ/m² |
ISO 179/1eU |
Résistance au choc Charpy (entaillé), +23°C, 3mm |
65 |
kJ/m² |
ISO 179/1eA |
Type de défaillance |
P |
- |
- |
Résistance au choc Charpy (entaillé), -30°C, 3mm |
14 |
kJ/m² |
ISO 179/1eA |
Type de défaillance |
C |
- |
- |
Résistance au choc Izod avec entaille, +23°C |
65 |
kJ/m² |
ISO 180/1A |
Résistance au choc Izod avec entaille |
15 |
kJ/m² |
ISO 180/1A |
Température |
-30 |
°C |
- |
Perforation - force maximum, +23°C |
5100 |
N |
ISO 6603-2 |
Perforation - force maximum, -30°C |
6000 |
N |
ISO 6603-2 |
Perforation - Energie, +23°C |
55 |
J |
ISO 6603-2 |
Perforation - Energie, -30°C |
65 |
J |
ISO 6603-2 |
Ball indentation hardness |
115 |
MPa |
ISO 2039-1 |
Propriétés thermiques | Valeur | Unité | Norme du test |
ISO Data |
Température de transition vitreuse, 10°C/min |
144 |
°C |
ISO 11357-1/-2 |
Température de fléchissement s/chrg, 1.80 MPa |
124 |
°C |
ISO 75-1/-2 |
Température de fléchissement s/chrg, 0.45 MPa |
137 |
°C |
ISO 75-1/-2 |
Température de ramolliss. Vicat, B |
145 |
°C |
ISO 306 |
Coeffic. de dilatation therm. linéique, parallèle |
65 |
E-6/K |
ISO 11359-1/-2 |
Coeffic. de dilatation therm. linéique, perpend. |
65 |
E-6/K |
ISO 11359-1/-2 |
Inflammabilité pr. épaisseur h |
V-2 |
class |
IEC 60695-11-10 |
Epaisseur de l'éprouvette |
0.8 |
mm |
- |
Aptitude à l'allumage |
27 |
% |
ISO 4589-1/-2 |
Glow Wire Flammability Index (GWFI) |
850 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (1) |
0.75 |
mm |
- |
Glow Wire Flammability Index (GWFI) |
875 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (2) |
1.5 |
mm |
- |
Glow Wire Flammability Index (GWFI) |
930 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (3) |
3 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (1) |
0.75 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (2) |
1 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (3) |
1.5 |
mm |
- |
Propriétés électriques | Valeur | Unité | Norme du test |
ISO Data |
Permittivité relative, 100Hz |
3.1 |
- |
IEC 62631-2-1 |
Permittivité relative, 1MHz |
3 |
- |
IEC 62631-2-1 |
Facteur de pertes, 100Hz |
5 |
E-4 |
IEC 62631-2-1 |
Facteur de pertes, 1MHz |
90 |
E-4 |
IEC 62631-2-1 |
Résistivité transversale |
>1E13 |
Ohm*m |
IEC 62631-3-1 |
Résistivité superficielle |
>1E15 |
Ohm |
IEC 62631-3-2 |
Rigidité diélectrique |
34 |
kV/mm |
IEC 60243-1 |
Indice de résistance au cheminement |
250 |
- |
IEC 60112 |
Propriétés optiques | Valeur | Unité | Norme du test |
ISO Data |
Haze |
80 |
- |
ISO 14782 |
Transmittance |
89 |
% |
ISO 13468-1, -2 |
Propriétés diverses | Valeur | Unité | Norme du test |
Absorption d'eau |
0.3 |
% |
Sim. to ISO 62 |
Absorption d'humidité |
0.12 |
% |
Sim. to ISO 62 |
Masse volumique |
1200 |
kg/m³ |
ISO 1183 |
Bulk density |
660 |
kg/m³ |
- |
Propriétés mécaniques (Grades film) | Valeur | Unité | Norme du test |
ISO Data |
Perméabilité à la vapeur d'eau, 23°C/85%r.h. |
15 |
g/(m²*d) |
ISO 15106-1/-2 |
Epaisseur des eprouvettes |
0.1 |
mm |
- |
Préparation et conditionnement des éprouvettes | Valeur | Unité | Norme du test |
ISO Data |
Injection, température de la matière fondue |
280 |
°C |
ISO 294 |
Injection, température du moule |
80 |
°C |
ISO 294 |
Injection, vitesse d'injection |
200 |
mm/s |
ISO 294 |
Recommandations pour la transformation Moulage par injection | Valeur | Unité | Norme du test |
Pré-séchage - température |
120 |
°C |
- |
Pré-séchage - temps |
2 - 3 |
h |
- |
L'humidité de traitement |
≤0.02 |
% |
- |
Température de la matière fondue |
280 - 320 |
°C |
- |
Température du moule |
80 - 120 |
°C |
- |
Zone 1 |
250 - 260 |
°C |
- |
Zone 2 |
270 - 280 |
°C |
- |
Zone 3 |
280 - 290 |
°C |
- |
Température de la buse |
290 - 300 |
°C |
- |
Contre-pression |
5 - 15 |
MPa |
- |
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage
Propriétés spéciales
Transparent, Opaque, Translucent
Certifications
ISCC Plus
Applications
General Purpose
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.