Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Makrolon® 2405 RE - PC - Covestro Deutschland AG
Material Data Center offers the following functions for Makrolon® 2405 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Product Texts
- MVR (300 °C/1.2 kg) 19 cm³/10 min
- general purpose
- low viscosity
- easy release
Processing/Physical Characteristics | Value | Unit | Test Standard |
ISO Data |
Melt volume-flow rate, MVR |
19 |
cm³/10min |
ISO 1133 |
Temperature |
300 |
°C |
- |
Load |
1.2 |
kg |
- |
Melt flow index, MFI |
20 |
g/10min |
ISO 1133 |
Temperature |
300 |
°C |
- |
Load |
1.2 |
kg |
- |
Molding shrinkage, parallel |
0.7 |
% |
ISO 294-4, 2577 |
Molding shrinkage, normal |
0.7 |
% |
ISO 294-4, 2577 |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Tensile Modulus |
2400 |
MPa |
ISO 527 |
Yield stress |
65 |
MPa |
ISO 527 |
Yield strain |
6 |
% |
ISO 527 |
Nominal strain at break |
>50 |
% |
ISO 527 |
Flexural modulus, 23°C |
2350 |
MPa |
ISO 178 |
Flexural strength |
97 |
MPa |
ISO 178 |
Tensile creep modulus, 1h |
2200 |
MPa |
ISO 899-1 |
Tensile creep modulus, 1000h |
1900 |
MPa |
ISO 899-1 |
Charpy impact strength, +23°C |
N |
kJ/m² |
ISO 179/1eU |
Charpy notched impact strength, +23°C, 3mm |
65 |
kJ/m² |
ISO 179/1eA |
Type of failure |
P |
- |
- |
Charpy notched impact strength, -30°C, 3mm |
14 |
kJ/m² |
ISO 179/1eA |
Type of failure |
C |
- |
- |
Izod notched impact strength, +23°C |
65 |
kJ/m² |
ISO 180/1A |
Izod notched impact strength |
15 |
kJ/m² |
ISO 180/1A |
Temperature |
-30 |
°C |
- |
Puncture - maximum force, +23°C |
5100 |
N |
ISO 6603-2 |
Puncture - maximum force, -30°C |
6000 |
N |
ISO 6603-2 |
Puncture energy, +23°C |
55 |
J |
ISO 6603-2 |
Puncture energy, -30°C |
65 |
J |
ISO 6603-2 |
Ball indentation hardness |
115 |
MPa |
ISO 2039-1 |
Thermal properties | Value | Unit | Test Standard |
ISO Data |
Glass transition temperature, 10°C/min |
144 |
°C |
ISO 11357-1/-2 |
Temp. of deflection under load, 1.80 MPa |
124 |
°C |
ISO 75-1/-2 |
Temp. of deflection under load, 0.45 MPa |
137 |
°C |
ISO 75-1/-2 |
Vicat softening temperature, B |
145 |
°C |
ISO 306 |
Coeff. of linear therm. expansion, parallel |
65 |
E-6/K |
ISO 11359-1/-2 |
Coeff. of linear therm. expansion, normal |
65 |
E-6/K |
ISO 11359-1/-2 |
Burning Behav. at thickness h |
V-2 |
class |
IEC 60695-11-10 |
Thickness tested |
0.8 |
mm |
- |
Oxygen index |
27 |
% |
ISO 4589-1/-2 |
Glow Wire Flammability Index (GWFI) |
850 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (1) |
0.75 |
mm |
- |
Glow Wire Flammability Index (GWFI) |
875 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (2) |
1.5 |
mm |
- |
Glow Wire Flammability Index (GWFI) |
930 |
°C |
IEC 60695-2-12 |
GWFI - thickness tested (3) |
3 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (1) |
0.75 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (2) |
1 |
mm |
- |
Glow Wire Ignition Temperature (GWIT) |
875 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (3) |
1.5 |
mm |
- |
Electrical properties | Value | Unit | Test Standard |
ISO Data |
Relative permittivity, 100Hz |
3.1 |
- |
IEC 62631-2-1 |
Relative permittivity, 1MHz |
3 |
- |
IEC 62631-2-1 |
Dissipation factor, 100Hz |
5 |
E-4 |
IEC 62631-2-1 |
Dissipation factor, 1MHz |
90 |
E-4 |
IEC 62631-2-1 |
Volume resistivity |
>1E13 |
Ohm*m |
IEC 62631-3-1 |
Surface resistivity |
>1E15 |
Ohm |
IEC 62631-3-2 |
Electric strength |
34 |
kV/mm |
IEC 60243-1 |
Comparative tracking index |
250 |
- |
IEC 60112 |
Optical properties | Value | Unit | Test Standard |
ISO Data |
Haze |
80 |
- |
ISO 14782 |
Luminous transmittance |
89 |
% |
ISO 13468-1, -2 |
Other properties | Value | Unit | Test Standard |
Water absorption |
0.3 |
% |
Sim. to ISO 62 |
Humidity absorption |
0.12 |
% |
Sim. to ISO 62 |
Density |
1200 |
kg/m³ |
ISO 1183 |
Bulk density |
660 |
kg/m³ |
- |
Film Properties | Value | Unit | Test Standard |
ISO Data |
WVTR, 23°C/85%r.h. |
15 |
g/(m²*d) |
ISO 15106-1/-2 |
Thickness of specimen |
0.1 |
mm |
- |
Test specimen production | Value | Unit | Test Standard |
ISO Data |
Injection Molding, melt temperature |
280 |
°C |
ISO 294 |
Injection Molding, mold temperature |
80 |
°C |
ISO 294 |
Injection Molding, injection velocity |
200 |
mm/s |
ISO 294 |
Processing Recommendation Injection Molding | Value | Unit | Test Standard |
Pre-drying - Temperature |
120 |
°C |
- |
Pre-drying - Time |
2 - 3 |
h |
- |
Processing humidity |
≤0.02 |
% |
- |
Melt temperature |
280 - 320 |
°C |
- |
Mold temperature |
80 - 120 |
°C |
- |
Zone 1 |
250 - 260 |
°C |
- |
Zone 2 |
270 - 280 |
°C |
- |
Zone 3 |
280 - 290 |
°C |
- |
Nozzle temperature |
290 - 300 |
°C |
- |
Back pressure |
5 - 15 |
MPa |
- |
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Special Characteristics
Transparent, Opaque, Translucent
Certifications
ISCC Plus
Applications
General Purpose
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.