Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Genestar™ GW1458HF - PA9T-GF45 - Kuraray Co., Ltd.

Material Data Center offers the following functions for Genestar™ GW1458HF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Genestar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Genestar GW1458HF is a 45%GF grade developed for E&E applications. 


The main features of GW1458HF are:
 -Low warpage
 -Good flow-ability

GW1458HF is suitable for warpage-sensitive card connectors.
加工/物理特性价值单位Test Standard
ISO数据
模塑收缩率, 平行 0.2 % ISO 294-4, 2577
模塑收缩率, 垂直 0.7 % ISO 294-4, 2577
ASTM数据
熔融指数, MFI 90 g/10min ASTM D 1238
温度 320 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
拉伸强度 157 MPa ISO 527
断裂应力 157 MPa ISO 527
断裂伸长率 1.5 % ISO 527
弯曲模量, 23°C 12800 MPa ISO 178
弯曲强度 242 MPa ISO 178
简支梁缺口冲击强度, +23°C 16 kJ/m² ISO 179/1eA
ASTM数据
拉伸强度 150 MPa ASTM D 638
弯曲模量 13000 MPa ASTM D 790
弯曲强度 207 MPa ASTM D 790
悬臂梁缺口冲击强度, 1/8 in 130 J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 306 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 125 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 290 °C ISO 75-1/-2
ASTM数据
UL94 燃烧性 HB - UL 94
DTUL @ 264 psi 290 °C ASTM D 648
熔点 306 °C ASTM D 3418
玻璃化转变温度 125 °C ASTM E 1356
电性能价值单位Test Standard
ASTM数据
电介质强度, 短时 30 kV/mm ASTM D 149
体积电阻率 >1E15 Ohm*cm ASTM D 257
其它性能价值单位Test Standard
吸水性 0.12 % 类似ISO 62
密度 1500 kg/m³ ISO 1183
密度 1500 kg/m³ ASTM D 792
典型数据
加工方法
注塑
特殊性能
经热稳处理的/耐热的
特征
低翘曲, 可焊的
应用
电子电气
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.