Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 100ST NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 100ST NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 100ST is a super-toughened, high viscosity acetal homopolymer grade with superior impact resistance.  It is designed for highly stressed parts where outstanding toughness is essential.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 1.7 cm³/10min ISO 1133
温度 190 °C -
载荷 2.16 kg -
模塑收缩率, 平行 0.8 % ISO 294-4, 2577
模塑收缩率, 垂直 1.1 % ISO 294-4, 2577
ASTM数据
熔融指数, MFI 0.8 g/10min ASTM D 1238
温度 190 °C -
负载 2.16 kg -
模压收缩率, 平行 0.0105 mm/mm ASTM D 955
模压收缩率, TD 0.0115 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
拉伸模量 1400 MPa ISO 527
屈服应力 41 MPa ISO 527
屈服伸长率 30 % ISO 527
名义断裂伸长率 >50 % ISO 527
拉伸蠕变模量, 1h 1100 MPa ISO 899-1
拉伸蠕变模量, 1000h 550 MPa ISO 899-1
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 90 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 18 kJ/m² ISO 179/1eA
肖氏硬度D 70 - ISO 7619-1
ASTM数据
拉伸模量 1300 MPa ASTM D 638
拉伸强度 32 MPa ASTM D 638
屈服应力 45 MPa ASTM D 638
屈服伸长率 35 % ASTM D 638
断裂伸长率 150 % ASTM D 638
弯曲模量 1130 MPa ASTM D 790
洛克硬度 R 105 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in N J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 250 J/m ASTM D 256
温度 -40 °C -
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 178 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min -35 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 60 °C ISO 75-1/-2
热变形温度, 0.45 MPa 100 °C ISO 75-1/-2
线性热膨胀系数, 平行 130 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 140 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
ASTM数据
UL94 燃烧性 HB - UL 94
测试厚度 1.5 mm -
热释放速率, 平行 126 E-6/K ASTM D 696
热释放速率, 垂直 136 E-6/K ASTM D 696
DTUL @ 66 psi 124 °C ASTM D 648
DTUL @ 264 psi 61 °C ASTM D 648
熔点 178 °C ASTM D 3418
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 4.4 - IEC 62631-2-1
相对介电常数., 1MHz 3.8 - IEC 62631-2-1
体积电阻率 1E12 Ohm*m IEC 62631-3-1
表面电阻率 1E14 Ohm IEC 62631-3-2
相对漏电起痕指数 600 - IEC 60112
ASTM数据
电介质强度, 短时 20 kV/mm ASTM D 149
耗散因素, 1 MHz 0.027 - ASTM D 150
电介质常数, 1 MHz 4.2 - ASTM D 150
表面电阻率 2E14 Ohm ASTM D 257
体积电阻率 4E14 Ohm*cm ASTM D 257
其它性能价值单位Test Standard
吸水性 0.9 % 类似ISO 62
吸湿性 0.35 % 类似ISO 62
密度 1340 kg/m³ ISO 1183
吸水率, 24小时 0.44 % ASTM D 570
吸水率, 平衡 0.35 % ASTM D 570
密度 1340 kg/m³ ASTM D 792
函数
粘度-剪切速度 , Delrin® 100ST NC010, POM, DuPont
剪切应力-剪切速度 , Delrin® 100ST NC010, POM, DuPont
动态剪切模量-温度 , Delrin® 100ST NC010, POM, DuPont
动态E-模量-温度 , Delrin® 100ST NC010, POM, DuPont
应力-应变.  , Delrin® 100ST NC010, POM, DuPont
正割模量-应变.  , Delrin® 100ST NC010, POM, DuPont
应力-应变(等时的) 23°C, Delrin® 100ST NC010, POM, DuPont
蠕变模量-时间. 23°C, Delrin® 100ST NC010, POM, DuPont
蠕变曲线 23°C, Delrin® 100ST NC010, POM, DuPont
比容-温度(pvT) , Delrin® 100ST NC010, POM, DuPont
典型数据
加工方法
注塑, 管材挤出, 异型材挤出成型, 片材挤出成型, 电线挤出, 其它挤出成型, 表面涂层, 吹塑
供货形式
粒料, 自然色
添加剂
润滑剂, 脱模助剂
特殊性能
高冲击韧性的/经抗冲改性的
特征
可焊的, 均聚物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.