Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 100ST NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 100ST NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 100ST is a super-toughened, high viscosity acetal homopolymer grade with superior impact resistance.  It is designed for highly stressed parts where outstanding toughness is essential.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 1.7 cm³/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Contracción posterior al moldeo, paralelo 0.8 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.1 % ISO 294-4, 2577
ASTM Data
Índice de fluidez, MFI 0.8 g/10min ASTM D 1238
Temperatura 190 °C -
Carga 2.16 kg -
Contracción posterior al moldeo, paralelo 0.0105 mm/mm ASTM D 955
Contracción posterior al moldeo, normal 0.0115 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1400 MPa ISO 527
Esfuerzo de fluencia 41 MPa ISO 527
Alarg. en límite elástico 30 % ISO 527
Alarg. nominal a rotura >50 % ISO 527
Módulo de plastodeformación, 1h 1100 MPa ISO 899-1
Módulo de plastodeformación, 1000h 550 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 90 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 18 kJ/m² ISO 179/1eA
Dureza Shore D 70 - ISO 7619-1
ASTM Data
Módulo de tracción 1300 MPa ASTM D 638
Esfuerzo de tracción 32 MPa ASTM D 638
Esfuerzo de fluencia a tracción 45 MPa ASTM D 638
Alargamiento a la fluencia 35 % ASTM D 638
Alargamiento a la rotura 150 % ASTM D 638
Módulo de flexión 1130 MPa ASTM D 790
Dureza Rockwell R 105 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in N J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 250 J/m ASTM D 256
Temperatura -40 °C -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 178 °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min -35 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 60 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 100 °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 130 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 140 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Yellow Card disponible - -
ASTM Data
Combustibilidad UL 94 HB - UL 94
Espesores de probeta 1.5 mm -
Coeficiente de dilatación térmica, long. 126 E-6/K ASTM D 696
Coeficiente de dilatación térmica, normal 136 E-6/K ASTM D 696
Estabilidad al calor @ 66 psi 124 °C ASTM D 648
Estabilidad al calor @ 264 psi 61 °C ASTM D 648
Temperatura de fusión 178 °C ASTM D 3418
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 4.4 - IEC 62631-2-1
Constante dieléctrica, 1MHz 3.8 - IEC 62631-2-1
Resistividad volumétrica específica 1E12 Ohm*m IEC 62631-3-1
Resistividad superficial específica 1E14 Ohm IEC 62631-3-2
Indice comparativo de linea de fuga 600 - IEC 60112
ASTM Data
Resistencia dieléctrica, tiempo corto 20 kV/mm ASTM D 149
Factor de pérdidas dieléctricas, 1 MHz 0.027 - ASTM D 150
Constante dieléctrica, 1 MHz 4.2 - ASTM D 150
Resistividad superficial 2E14 Ohm ASTM D 257
Resistividad volumétrica 4E14 Ohm*cm ASTM D 257
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.9 % Sim. to ISO 62
Absorción de humedad 0.35 % Sim. to ISO 62
Densidad 1340 kg/m³ ISO 1183
Absorción de agua, 24hr 0.44 % ASTM D 570
Absorción de agua, equilibrio 0.35 % ASTM D 570
Densidad 1340 kg/m³ ASTM D 792
Funciones
Viscosidad-velocidad de cizallamiento , Delrin® 100ST NC010, POM, DuPont
Tensión de cizalla-velocidad de cizalla , Delrin® 100ST NC010, POM, DuPont
Módulo de cizallamiento dinámico-temperatura , Delrin® 100ST NC010, POM, DuPont
Módulo de tensión dinámico-temperatura , Delrin® 100ST NC010, POM, DuPont
Esfuerzo-alargamiento , Delrin® 100ST NC010, POM, DuPont
Módulo secante-alargamiento , Delrin® 100ST NC010, POM, DuPont
Esfuerzo-alargamiento (isocrono) 23°C, Delrin® 100ST NC010, POM, DuPont
Módulo de plastodeformación-tiempo 23°C, Delrin® 100ST NC010, POM, DuPont
Curva de creep 23°C, Delrin® 100ST NC010, POM, DuPont
Volumen especifico-temperatura (pvT) , Delrin® 100ST NC010, POM, DuPont
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusión de tubería, Extrusión de perfiles, Extrusión de láminas, Extrusión de cable, Otros tipos de extrusión, Recubrimiento, Moldeo por soplado
Forma de suministro
Sémola, Color natural
Aditivos
Lubricante, Desmoldeante
Características especiales
Alto impacto o modificado al impacto
Características
Soldable, Homopolímero
Disponibilidad regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.