Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 100AL NC010 - POM-Z - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 100AL NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 100AL is a high viscosity acetal homopolymer containing an advanced system of lubrication designed for low wear, low friction, and low noise against metals and plastics.
加工/物理特性价值单位Test Standard
ISO数据
模塑收缩率, 平行 2.0 % ISO 294-4, 2577
模塑收缩率, 垂直 1.7 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 3000 MPa ISO 527
屈服应力 70 MPa ISO 527
屈服伸长率 18 % ISO 527
名义断裂伸长率 40 % ISO 527
拉伸蠕变模量, 1h 2700 MPa ISO 899-1
拉伸蠕变模量, 1000h 1500 MPa ISO 899-1
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 200 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 10.5 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 7.5 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 178 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 97 °C ISO 75-1/-2
热变形温度, 0.45 MPa 163 °C ISO 75-1/-2
线性热膨胀系数, 平行 110 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 110 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
Yellow Card 现存 是的 - -
其它性能价值单位Test Standard
密度 1400 kg/m³ ISO 1183
函数
粘度-剪切速度 , Delrin® 100AL NC010, POM-Z, DuPont
剪切应力-剪切速度 , Delrin® 100AL NC010, POM-Z, DuPont
应力-应变.  , Delrin® 100AL NC010, POM-Z, DuPont
正割模量-应变.  , Delrin® 100AL NC010, POM-Z, DuPont
比容-温度(pvT) , Delrin® 100AL NC010, POM-Z, DuPont
典型数据
加工方法
注塑, 异型材挤出成型, 片材挤出成型, 其它挤出成型
供货形式
粒料, 自然色
添加剂
润滑剂, 脱模助剂
特征
均聚物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

耐化学性
酸类
醋酸 (5g/100g) (23°C)
柠檬酸溶液 (10g/100g) (23°C)
乳酸 (10g/100g) (23°C)
盐酸 (36g/100g) (23°C)
硝酸 (40g/100g) (23°C)
硫酸 (38g/100g) (23°C)
硫酸 (5g/100g) (23°C)
铬酸溶液 (40g/100g) (23°C)
碱类
氢氧化钠溶液 (35g/100g) (23°C)
氢氧化钠溶液 (1g/100g) (23°C)
氨水(氢氧化铵) (10g/100g) (23°C)
醇类
异丙醇 (23°C)
甲醇 (23°C)
乙醇 (23°C)
碳氢化合物
正乙烷 (23°C)
甲苯 (23°C)
异辛烷 (23°C)
酮类
丙酮 (23°C)
醚类
(二)乙醚 (23°C)
矿物油
SAE 10W40号多效润滑油 (23°C)
SAE 10W40号多效润滑油 (130°C)
SAE 89/90号变速箱润滑油 (130°C)
绝缘油 (23°C)
滑油OS206 304 Ref.Eng.Oil, ISP (135°C)
自动准双曲面齿轮油壳牌壳牌Donax (135°C)
水力油Pentosin CHF 202 (125°C)
标准燃油
ISO 1817 燃油1号 (60°C)
ISO 1817 燃油2号 (60°C)
ISO 1817 燃油3号 (60°C)
ISO 1817 燃油4号 (60°C)
不含酒精的标准燃油(优先使用C类ISO 1817 燃油) (23°C)
含酒精的标准燃油(优先使用4号ISO 1817 燃油) (23°C)
柴油(优先使用F类ISO 1817液体) (23°C)
柴油(优先使用F类ISO 1817液体) (90°C)
柴油(优先使用F类ISO 1817液体) (>90°C)
盐溶液
氯化钠溶液(10g/100g) (23°C)
次氯化钠溶液 (10g/100g) (23°C)
碳酸钠溶液 (20g/100g) (23°C)
碳酸钠溶液 (2g/100g) (23°C)
氯化锌溶液 (50g/100g) (23°C)
其它
乙酸乙酯 (23°C)
过氧化氢 (23°C)
DOT4号刹车油 (130°C)
乙二醇水溶液 (50g/100g) (108°C)
1g/100g 基苯氧- 聚环氧乙烷乙烯水溶液 (23°C)
油酸 (50g/100g) + 橄榄油 (50g/100g) (23°C)
水 (23°C)
去离子水 (90°C)
酚溶液(5g/100g) (23°C)
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.