Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 100AL NC010 - POM-Z - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 100AL NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 100AL is a high viscosity acetal homopolymer containing an advanced system of lubrication designed for low wear, low friction, and low noise against metals and plastics.
Processing/Physical Characteristics単位テスト基準
ISO データ
成形収縮率, 平行 2.0 % ISO 294-4, 2577
成形収縮率, 直角 1.7 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 3000 MPa ISO 527
降伏応力 70 MPa ISO 527
降伏ひずみ 18 % ISO 527
破壊呼びひずみ 40 % ISO 527
引張クリープ弾性率, 1h 2700 MPa ISO 899-1
引張クリープ弾性率, 1000h 1500 MPa ISO 899-1
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 200 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 10.5 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 7.5 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 178 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 97 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 163 °C ISO 75-1/-2
線膨張係数, 平行 110 E-6/K ISO 11359-1/-2
線膨張係数, 直角 110 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
Yellow Card 可用 はい - -
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 0.8 mm -
Yellow Card 可用 はい - -
その他の特性.単位テスト基準
密度 1400 kg/m³ ISO 1183
機能
 粘度せん断速度. , Delrin® 100AL NC010, POM-Z, DuPont
 せん断応力-せん断速度. , Delrin® 100AL NC010, POM-Z, DuPont
 応力-ひずみ. , Delrin® 100AL NC010, POM-Z, DuPont
 割線弾性率−ひずみ. , Delrin® 100AL NC010, POM-Z, DuPont
 pvT , Delrin® 100AL NC010, POM-Z, DuPont
特殊な特性
成形加工法.
射出成形., 異形押出成形., シート押出成形., その他の押出成形.
納入形状.
ペレット., ナチュラルカラー
添加剤.
滑剤., 離型剤.
な特性
Homopolymer
領域別の利用可能性
その他の情報
村遜速揃
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

耐薬品性
5wt%酢酸 (23゚C)
10wt%クエン酸 (23゚C)
10wt%乳酸 (23゚C)
36wt%塩酸 (23゚C)
40wt%硝酸 (23゚C)
38wt%硫酸 (23゚C)
5wt%硫酸 (23゚C)
40wt%硝酸 (23゚C)
塩基
35wt%水酸化ナトリウム (23゚C)
1wt%水酸化ナトリウム (23゚C)
10wt%水酸化アンモニウム (23゚C)
アルコール
イソプロピルアルコール23℃ (23゚C)
メタノール 23℃ (23゚C)
エタノール 23℃ (23゚C)
炭化水素
ヘキサン (23゚C)
トルエン (23゚C)
イソオクタン (23゚C)
ケトン系溶剤
アセトン (23゚C)
エーテル溶剤
ジエチルエーテル (23゚C)
鉱油
SAE 10W40 マルチグレードモーターオイル (23゚C)
SAE 10W40 マルチグレードモーターオイル (130゚C)
SAE 80/90 ハイポイドギアオイル (130゚C)
絶縁油 (23゚C)
モーターオイルOS206 304 Ref.Eng.Oil, ISP (135゚C)
ハイポイドギアオイルShell Donax TX (135゚C)
油圧オイル Pentosin CHF 202 (125゚C)
標準燃料
ISO 1817液1 (60゚C)
ISO 1817液2 (60゚C)
ISO 1817液3 60℃ (60゚C)
ISO 1817液4 (60゚C)
標準燃料(ISO 1817液C)アルコールなし (23゚C)
標準燃料(ISO 1817液4)アルコールあり (23゚C)
ディーゼル燃料(ISO 1817液F) (23゚C)
ディーゼル燃料(ISO 1817液F) (90゚C)
ディーゼル燃料(ISO 1817液F) (>90゚C)
食塩水
10wt%塩化ナトリウム (23゚C)
10wt%次亜塩素酸ナトリウム (23゚C)
20wt%炭酸ナトリウム (23゚C)
2wt%炭酸ナトリウム (23゚C)
50wt%ジンクロメート (23゚C)
その他
エチルアセテート (23゚C)
過酸化水素 (23゚C)
DOT No.4ブレーキ液 (130゚C)
50wt%エチレングリコール水溶液 (108゚C)
1wt%ノニルフェノキシ-ポリエチレノキシ-エタノール水... (23゚C)
オレイン酸50%+オリーブオイル50% (23゚C)
水 (23゚C)
純水 (90゚C)
5wt%フェノール溶液 (23゚C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com