Características de processamento/físicas | Valor | Unidade | Método de ensaio |
Other Standards[S] |
Contração após a moldagem, paralelo |
0.0049 |
mm/mm |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriedades mecânicas | Valor | Unidade | Método de ensaio |
Other Standards[S] |
Res. impacto Charpy c/entalhe, +23°C |
3.1 |
kJ/m² |
JIS K 6911 |
Módulo de flexão |
9500 |
MPa |
JIS K 6911 |
Resistência à flexão |
102 |
MPa |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriedades térmicas | Valor | Unidade | Método de ensaio |
ASTM Dados |
UL94 flamabilidade |
V-0 |
- |
UL 94 |
Espessuras do tubo de teste |
0.43 |
mm |
- |
Other Standards[S] |
DTUL @ 264 psi |
225 |
°C |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriedades elétricas | Valor | Unidade | Método de ensaio |
ISO Dados |
Índice comparativo de linha de fuga |
175 |
- |
IEC 60112 |
Other Standards[S] |
Resistência elétrica, step/step |
10 |
kV/mm |
JIS K 6911 |
Resistência ao arco |
180 |
s |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Outras propriedades | Valor | Unidade | Método de ensaio |
Other Standards[S] |
Densidade |
1670 |
kg/m³ |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Características
Processamento
Moldagem por injeção, Moldagem por transferência
Forma de entrega
Negro
Características especiais
Estável contra o calor
Certifications
Contém recursos renováveis
Aplicaciones
Elétrica e Eletrônica
Disponibilidade regional
América do Norte
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.