Processing/Physical Characteristics | Value | Unit | Test Standard |
Other Standards[S] |
Mold Shrinkage, MD |
0.0049 |
mm/mm |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Mechanical properties | Value | Unit | Test Standard |
Other Standards[S] |
Charpy notched impact strength, +23°C |
3.1 |
kJ/m² |
JIS K 6911 |
Flexural Modulus |
9500 |
MPa |
JIS K 6911 |
Flexural Strength |
102 |
MPa |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Thermal properties | Value | Unit | Test Standard |
ASTM Data |
UL 94 Flame rating |
V-0 |
- |
UL 94 |
Thickness tested |
0.43 |
mm |
- |
Other Standards[S] |
DTUL @ 264 psi |
225 |
°C |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Electrical properties | Value | Unit | Test Standard |
ISO Data |
Comparative tracking index |
175 |
- |
IEC 60112 |
Other Standards[S] |
Dielectric Strength, Step-by-Step |
10 |
kV/mm |
JIS K 6911 |
Arc Resistance |
180 |
s |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Other properties | Value | Unit | Test Standard |
Other Standards[S] |
Density |
1670 |
kg/m³ |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Characteristics
Processing
Injection Molding, Transfer Molding
Delivery form
Black
Special Characteristics
Heat stabilized or stable to heat
Certifications
Contains renewable resources
Applications
Electrical and Electronical
Regional Availability
North America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com