Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Resist zk50 - PMMA-I - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Resist zk50:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

Productprofil:

PLEXIGLAS® Resist zk50 is an amorphous, impact-modified thermoplastic molding compound (PMMA-I).

 

Typical properties of impact-modified PLEXIGLAS® molding compounds are

 

  • excellent transmission and clarity
  • brilliant appearance
  • the pleasant feel and sound of the moldings.

 

PLEXIGLAS® Resist zk50 is characterized by the following special properties:

 

  • maximum break resistance and impact strength
  • improved resistance to stress cracking
  • certified dishwasher resistance

Application:

Used for injection molding. Profile extrusion or coextrusion are also possible

Example:

lighting fixtures, writing and drawing utensils, domestic appliances and sanitaryware

Processing:

PLEXIGLAS® Resist zk molding compounds can be processed on machines with 3-zone general purpose screws for engineering thermoplastics.

Physical Form / Packaging:

PLEXIGLAS® Resist zk molding compounds are supplied as pellets of uniform size, packaged in 25kg polyethylene bags or 500kg boxes with PE lining; other packaging on request.

Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 0.1 cm³/10min ISO 1133
온도 230 °C -
하중 3.8 kg -
용융 밀도 1040 kg/m³ -
용융 열전도율 0.19 W/(m K) -
용융 비열용량 2440 J/(kg K) -
효율적 열전도도 7.49E-8 m²/s -
이형온도 55 °C -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 950 MPa ISO 527
항복강도 25 MPa ISO 527
항복변형률 5 % ISO 527
파단시 평균신율 >50 % ISO 527
탄성변형률, 1h 900 MPa ISO 899-1
탄성변형률, 1000h 600 MPa ISO 899-1
챠피 충격 강도 , +23°C N kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 13 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
유리 전이 온도, 10 °C/min 115 °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 70 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 73 °C ISO 75-1/-2
비카트 연화 온도, B 75 °C ISO 306
선형 열팽창 계수, 평행 150 E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.6 mm -
Yellow Card 유효한 - -
산소지수로서의 난연성 17.5 % ISO 4589-1/-2
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 4 - IEC 62631-2-1
상대 유전뮬, 1MHz 2.9 - IEC 62631-2-1
소산 인자, 100Hz 400 E-4 IEC 62631-2-1
소산 인자, 1MHz 400 E-4 IEC 62631-2-1
부피 저항 >1E13 Ohm*m IEC 62631-3-1
표면 저항 1E13 Ohm IEC 62631-3-2
CTI 600 - IEC 60112
광학 특성단위시험규격
ISO Data
광선 투겠淅 89 % ISO 13468-1, -2
기타 특성단위시험규격
물에서의 흡수성 1.2 % ISO 62와 유사
조건에서의 흡습성 0.4 % ISO 62와 유사
밀도 1120 kg/m³ ISO 1183
테스트 견본 생산단위시험규격
ISO 데이터
사출성형: 용융수지온도 265 °C ISO 294
사출성형: 금형온도 40 °C ISO 294
사출성형: 사출속도 195 mm/s ISO 294
도표
점도-변형률 , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
전단-변형률 , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
동전단탄성율-온도 , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
응력-신율 , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
시컨트탄성율-신율 , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
응력-신율(등시) 23°C, PLEXIGLAS® Resist zk50, PMMA-I, Röhm
크립탄성율-시간 23°C, PLEXIGLAS® Resist zk50, PMMA-I, Röhm
곡선 크리프 23°C, PLEXIGLAS® Resist zk50, PMMA-I, Röhm
인장탄성율-온도 , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
특징
생산 공정
사출 성형, 필름 압출, 외형 압출, 시트 압출, 기타 압출
인도 유형
펠렛 (입자,알갱이)
부가물
이형제
특별 특성
고충격 또는 고충격 보강, 가시광선 안정성, U.V. 안정성 또는 기후 안정성, 투명도
특성
Amorphous
내화학성에
Environmental Stress Crack Resistance
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
기타 정보
사E성
PREPROCESSING
Predrying temperature: max. 70 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 230 - 240°C
Mold temperature:50 - 70°C
프로파일 압
PREPROCESSING
Predrying temperature: max. 70 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 230 - 240 °C
Die temperature: 230 - 240 °C
시트 압
PREPROCESSING
Predrying temperature: max. 70 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 230 - 240 °C
Die temperature: 230 - 240 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com