Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ULTEM™ Resin 3310TD - PEI - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for ULTEM™ Resin 3310TD:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultem datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
ULTEM 3310TD resin is an amorphous, filled, near infra-red transparent polyetherimide (PEI) thermoplastic, offering a material with an unique combination of low CTE and high near infra-red transparency.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 6.84 cm³/10min ISO 1133
温度 337 °C -
荷重 6.7 kg -
ASTM数据
メルトフローレイト, MFI 10.3 g/10min ASTM D 1238
温度 337 °C -
荷重 6.7 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 4900 MPa ISO 527
破壊応力 67 MPa ISO 527
破壊ひずみ 1.6 % ISO 527
曲げ弾性率, 23°C 4900 MPa ISO 178
シャルピー衝撃強さ, +23°C 21.1 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 4.1 kJ/m² ISO 179/1eA
アイゾット衝撃試験, +23°C 36.5 kJ/m² ISO 180/1U
ノッチ付きIzod衝撃強さ, +23°C 4.7 kJ/m² ISO 180/1A
ASTM数据
引張弾性率 5000 MPa ASTM D 638
破壊応力 62 MPa ASTM D 638
破断伸び 1.5 % ASTM D 638
曲げ弾性率 5000 MPa ASTM D 790
曲げ強さ 109 MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 47 J/m ASTM D 256
アイゾット衝撃試験, 1/8 in 580 J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 197 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 208 °C ISO 75-1/-2
ビカット軟化温度, B 211 °C ISO 306
ASTM数据
線膨張係数, 平行 39 E-6/K ASTM D 696
線膨張係数, 直角 40 E-6/K ASTM D 696
DTUL @ 66 psi 206 °C ASTM D 648
DTUL @ 264 psi 196 °C ASTM D 648
ビカット軟化温度 211 °C ASTM D 1525
その他の特性.単位テスト基準
吸湿率 0.077 % Sim. to ISO 62
密度. 1540 kg/m³ ISO 1183
密度 1550 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 135 - 150 °C -
Pre-drying - Time 4 - 6 h -
Processing humidity ≤0.02 % -
樹脂温度 360 - 390 °C -
金型温度 150 - 190 °C -
Zone 1 350 - 370 °C -
Zone 2 350 - 370 °C -
Zone 3 350 - 380 °C -
Nozzle temperature 350 - 380 °C -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
熱安定化., 透明.
な特性
Amorphous
アプリケーション
電気電子
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.