Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ULTEM™ Resin 3310TD - PEI - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for ULTEM™ Resin 3310TD:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultem datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
ULTEM 3310TD resin is an amorphous, filled, near infra-red transparent polyetherimide (PEI) thermoplastic, offering a material with an unique combination of low CTE and high near infra-red transparency.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 6.84 cm³/10min ISO 1133
Température 337 °C -
Charge 6.7 kg -
ASTM Data
Indice de fluidité, MFI 10.3 g/10min ASTM D 1238
Température 337 °C -
Charge 6.7 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 4900 MPa ISO 527
Contrainte à la rupture 67 MPa ISO 527
Déformation à la rupture 1.6 % ISO 527
Module de flexion, 23°C 4900 MPa ISO 178
Résistance au choc Charpy, +23°C 21.1 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 4.1 kJ/m² ISO 179/1eA
Résistance au choc Izod, +23°C 36.5 kJ/m² ISO 180/1U
Résistance au choc Izod avec entaille, +23°C 4.7 kJ/m² ISO 180/1A
ASTM Data
Module en traction 5000 MPa ASTM D 638
Résistance de traction à la rupture 62 MPa ASTM D 638
Allongement à la rupture 1.5 % ASTM D 638
Module de flexion 5000 MPa ASTM D 790
Résistance à la flexion 109 MPa ASTM D 790
Izod choc avec entaille, 1/8 in 47 J/m ASTM D 256
Résistance au choc Izod, 1/8 in 580 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 197 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 208 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 211 °C ISO 306
ASTM Data
coefficient de dilatation thermique, long. 39 E-6/K ASTM D 696
Coefficient de dilatation thermique, trav. 40 E-6/K ASTM D 696
DTUL à 66 psi 206 °C ASTM D 648
DTUL à 264 psi 196 °C ASTM D 648
Vicat température 211 °C ASTM D 1525
Propriétés diversesValeurUnitéNorme du test
Absorption d'humidité 0.077 % Sim. to ISO 62
Masse volumique 1540 kg/m³ ISO 1183
Densité 1550 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 135 - 150 °C -
Pré-séchage - temps 4 - 6 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 360 - 390 °C -
Température du moule 150 - 190 °C -
Zone 1 350 - 370 °C -
Zone 2 350 - 370 °C -
Zone 3 350 - 380 °C -
Température de la buse 350 - 380 °C -
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Stabilisé à la chaleur, Transparent
Caractéristiques
Amorphe
Applications
Électrotechnique et électrique
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.