Caratteristiche Fisiche | Valore | Unitá | Norma del test |
Other Standards[S] |
Ritiro di stampaggio, parallelo |
0.0049 |
mm/mm |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Meccaniche | Valore | Unitá | Norma del test |
Other Standards[S] |
Resist. urto Charpy con intaglio, +23°C |
3.1 |
kJ/m² |
JIS K 6911 |
Modulo a flessione |
9500 |
MPa |
JIS K 6911 |
Resistenza alla flessione |
102 |
MPa |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Termiche | Valore | Unitá | Norma del test |
ASTM Data |
UL 94 combustibilitá |
V-0 |
- |
UL 94 |
Spessore testati |
0.43 |
mm |
- |
Other Standards[S] |
DTUL a 264 psi |
225 |
°C |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Elettriche | Valore | Unitá | Norma del test |
ISO Data |
Res. Alle correnti striscianti superficiali |
175 |
- |
IEC 60112 |
Other Standards[S] |
Rigidità dielettrica, step/step |
10 |
kV/mm |
JIS K 6911 |
Resistenza all’arco |
180 |
s |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Altre Proprietà | Valore | Unitá | Norma del test |
Other Standards[S] |
Densità |
1670 |
kg/m³ |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Stampaggio a Trasferimento
Forma fisica disponibile
Nero
Caratteristiche speciali
Stabilizzato o stabile al calore
Certifications
Contiene risorse rinnovabili
Applicazioni
Elettrotecnica ed electrici
Disponibilità geografica
Nord America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.