Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 100AL NC010 - POM-Z - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 100AL NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 100AL is a high viscosity acetal homopolymer containing an advanced system of lubrication designed for low wear, low friction, and low noise against metals and plastics.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 2.0 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.7 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3000 MPa ISO 527
Carico unitario a trazione 70 MPa ISO 527
Deformazione a snervamento 18 % ISO 527
Deformazione nominale a rottura 40 % ISO 527
Modulo di scorrimento a trazione, 1h 2700 MPa ISO 899-1
Modulo di scorrimento a trazione, 1000h 1500 MPa ISO 899-1
Resistenza all'urto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 200 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 10.5 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 7.5 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 178 °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 97 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 163 °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 110 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 110 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
Yellow Card disponibile - -
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 0.8 mm -
Yellow Card disponibile - -
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1400 kg/m³ ISO 1183
Funzioni
Viscosità-Velocità di taglio , Delrin® 100AL NC010, POM-Z, DuPont
Sforzo di taglio-Velocità di taglio , Delrin® 100AL NC010, POM-Z, DuPont
Sforzi-deformazione , Delrin® 100AL NC010, POM-Z, DuPont
Modulo secante-deformazione , Delrin® 100AL NC010, POM-Z, DuPont
Volume specifico-temperatura (pvT) , Delrin® 100AL NC010, POM-Z, DuPont
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Profilati, Estrusione di Lastre/Fogli, Altre Estrusioni
Forma fisica disponibile
Pellet, Colore naturale
Additivi
Lubrificanti, Agente di distacco
Caratteristiche
Omopolimero
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

Resistenza chimica
Acidi
Acido acetico (5% da massa) (23°C)
Soluzione acida citrica (10% da massa) (23°C)
Acido lattico (10% da massa) (23°C)
Acido cloridrico (36% da massa) (23°C)
Acido nitrico (40% da massa) (23°C)
Acido solforico (38% da massa) (23°C)
Acido solforico (5% da massa) (23°C)
Soluzione acida cromica (40% da massa) (23°C)
Basi
Soluzione dell' idrossido del sodio (35% da massa) (23°C)
Soluzione dell' idrossido del sodio (1% da massa) (23°C)
Soluzione dell' idrossido di ammonio (10% da massa) (23°C)
Alcool
Alcool di isopropile (23°C)
Metanolo (23°C)
Etanolo (23°C)
Idrocarburi
n-Hexane (23°C)
Toluene (23°C)
isoottano (23°C)
Chetoni
Acetone (23°C)
Eteri
Etere Etilico (23°C)
Oli minerali
Olio multigrade del motore di SAE 10W40 (23°C)
Olio multigrade del motore di SAE 10W40 (130°C)
Olio dell' ipoide-ingranaggio di SAE 80/90 (130°C)
Olio isolante (23°C)
Olio motore OS206 304 Ref.Eng.Oil, ISP (135°C)
Olio per cambio automatico Shell Donax TX (135°C)
Olio idraulico Pentosin CHF 202 (125°C)
Combustibili Standard
Liquido 1 di ISO 1817 (60°C)
Liquido 2 di ISO 1817 (60°C)
Liquido 3 di ISO 1817 (60°C)
Liquido 4 di ISO 1817 (60°C)
Combust. stand. senza alcool (pref. ISO 1817 liquido C) (23°C)
Combust. stand. con alcool (pref. ISO 1817 liquido 4) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (90°C)
Combustibile diesel (pref. ISO 1817 liquido F) (>90°C)
Soluzioni saline
Soluzione del cloruro di sodio (10% da massa) (23°C)
Soluzione dell' ipoclorito del sodio (10% da massa) (23°C)
Soluzione del carbonato di sodio (20% da massa) (23°C)
Soluzione del carbonato di sodio (2% da massa) (23°C)
Soluzione del cloruro dello zinco (50% da massa) (23°C)
Altri
Acetato etilico (23°C)
Perossido di idrogeno (23°C)
Liquido di freno del DOT N° 4 (130°C)
Glicol etilenico (50% da massa) in acqua (108°C)
etanolo di nonylphenoxy-polyethyleneoxy 1% in acqua (23°C)
acido oleico 50% + olio di oliva 50% (23°C)
Acqua (23°C)
Acqua deionizzata (90°C)
Soluzione del fenolo (5% da massa) (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.