Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test |
Other Standards[S] |
Retrait au moulage , parallèle |
0.0049 |
mm/mm |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés mécaniques | Valeur | Unité | Norme du test |
Other Standards[S] |
Résistance au choc Charpy (entaillé), +23°C |
3.1 |
kJ/m² |
JIS K 6911 |
Module de flexion |
9500 |
MPa |
JIS K 6911 |
Résistance à la flexion |
102 |
MPa |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés thermiques | Valeur | Unité | Norme du test |
ASTM Data |
UL 94 inflammabilité |
V-0 |
- |
UL 94 |
Épaisseur testée |
0.43 |
mm |
- |
Other Standards[S] |
DTUL à 264 psi |
225 |
°C |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés électriques | Valeur | Unité | Norme du test |
ISO Data |
Indice de résistance au cheminement |
175 |
- |
IEC 60112 |
Other Standards[S] |
Rigidité diélectrique, step/step |
10 |
kV/mm |
JIS K 6911 |
Résistance à l’arc |
180 |
s |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés diverses | Valeur | Unité | Norme du test |
Other Standards[S] |
Densité |
1670 |
kg/m³ |
JIS K 6911 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Caractéristiques
Transformation
Moulage par injection, Moulage par transfert
Conditionnement
Noir
Propriétés spéciales
Stabilisé à la chaleur
Certifications
Contient des ressources renouvelables
Applications
Électrotechnique et électrique
Disponibilité régionale
Amérique du nord
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com