Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DuraForm® PA Plastic - PA12 - 3D Systems Corporation

Material Data Center offers the following functions for DuraForm® PA Plastic:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Duraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module en traction 1586 MPa ASTM D 638
Module de traction 43 MPa ASTM D 638
Allongement à la rupture 14 % ASTM D 638
Module de flexion 1386 MPa ASTM D 790
Résistance à la flexion 48 MPa ASTM D 790
Dureté D Shore 73 - ASTM D 2240
Gardner au choc 2.71 J ASTM D 2794,4226,5420
Izod choc avec entaille, 1/8 in 32 J/m ASTM D 256
Résistance au choc Izod, 1/8 in 336 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
UL 94 inflammabilité HB - UL 94
DTUL à 66 psi 180 °C ASTM D 648
DTUL à 264 psi 95 °C ASTM D 648
Other Standards[S]
coefficient de dilatation thermique, long. 82.8 E-6/K ASTM E 831
Chaleur spécifique 1040 J/(kg K) ASTM E 1269
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés électriquesValeurUnitéNorme du test
ASTM Data
Rigidité diélectrique, peu de temps 17.3 kV/mm ASTM D 149
Résistance de la surface 7E12 Ohm ASTM D 257
Résistance volumique 5.9E13 Ohm*cm ASTM D 257
Propriétés diversesValeurUnitéNorme du test
Absorption d’eau, 24hr 0.07 % ASTM D 570
Densité 1000 kg/m³ ASTM D 792
Caractéristiques
Transformation
Additive Manufacturing
Conditionnement
Poudre, Blanc
Propriétés spéciales
Stérilisable, Stérilisation à la vapeur
Résistance Chimique
Résistance chimique générale
Certifications
Grade médical, USP Class VI approbation
Applications
Avions et aéronautique, Électrotechnique et électrique, Médical
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.