Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PPcompound 19T1040 - PP - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PPcompound 19T1040:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
SABIC® PPcompound 19T1040 is a 40% talc-filled polypropylene homopolymer. The material's high fill grade makes for a very high stiffness. This combined with the high flow and good thermal stabilization makes it especially suited for complex injection molded applications requiring a very high modulus and high thermal stability. SABIC® PPcompound 19T1040 is a designated automotive grade. IMDS ID: 16488039
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Índice de fluidez, MFI 18 g/10min ISO 1133
Temperatura 230 °C -
Carga 2.16 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 3600 MPa ISO 527
Esfuerzo de fluencia 30 MPa ISO 527
Alarg. en límite elástico 2.3 % ISO 527
Resistencia a la tracción 24 MPa ISO 527
Alargamiento a rotura 11 % ISO 527
Módulo de flexión, 23°C 3600 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 3 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 1 kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla 1.5 kJ/m² ISO 180/1A
ASTM Data
Módulo de tracción 3990 MPa ASTM D 638
Esfuerzo de fluencia a tracción 32 MPa ASTM D 638
Esfuerzo de fractura a tracción 28 MPa ASTM D 638
Alargamiento a la fluencia 3 % ASTM D 638
Alargamiento a la rotura 6.7 % ASTM D 638
Módulo de flexión 3600 MPa ASTM D 790
Dureza D Shore 75 - ASTM D 2240
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 89 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 130 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, A 150 °C ISO 306
ASTM Data
Estabilidad al calor @ 66 psi 134 °C ASTM D 648
Estabilidad al calor @ 264 psi 78 °C ASTM D 648
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1250 kg/m³ ISO 1183
Densidad 1260 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 - 100 °C -
Tiempo de pre-secado 2 - 4 h -
Temperatura de la masa 210 - 270 °C -
Temperatura del molde 15 - 60 °C -
Zona 1 190 - 230 °C -
Zona 2 200 - 250 °C -
Zona 3 210 - 270 °C -
Temperatura de boquilla 210 - 270 °C -
Contrapresión 1 - 1.5 MPa -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Características
Homopolímero
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.