Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Resist zk50 - PMMA-I - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Resist zk50:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Productprofil:

PLEXIGLAS® Resist zk50 is an amorphous, impact-modified thermoplastic molding compound (PMMA-I).

 

Typical properties of impact-modified PLEXIGLAS® molding compounds are

 

  • excellent transmission and clarity
  • brilliant appearance
  • the pleasant feel and sound of the moldings.

 

PLEXIGLAS® Resist zk50 is characterized by the following special properties:

 

  • maximum break resistance and impact strength
  • improved resistance to stress cracking
  • certified dishwasher resistance

Application:

Used for injection molding. Profile extrusion or coextrusion are also possible

Example:

lighting fixtures, writing and drawing utensils, domestic appliances and sanitaryware

Processing:

PLEXIGLAS® Resist zk molding compounds can be processed on machines with 3-zone general purpose screws for engineering thermoplastics.

Physical Form / Packaging:

PLEXIGLAS® Resist zk molding compounds are supplied as pellets of uniform size, packaged in 25kg polyethylene bags or 500kg boxes with PE lining; other packaging on request.

Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 0.1 cm³/10min ISO 1133
Temperature 230 °C -
Load 3.8 kg -
Density of melt 1040 kg/m³ -
Thermal conductivity of melt 0.19 W/(m K) -
Spec. heat capacity of melt 2440 J/(kg K) -
Eff. thermal diffusivity 7.49E-8 m²/s -
Ejection temperature 55 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 950 MPa ISO 527
Yield stress 25 MPa ISO 527
Yield strain 5 % ISO 527
Nominal strain at break >50 % ISO 527
Tensile creep modulus, 1h 900 MPa ISO 899-1
Tensile creep modulus, 1000h 600 MPa ISO 899-1
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 13 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min 115 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 70 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 73 °C ISO 75-1/-2
Vicat softening temperature, B 75 °C ISO 306
Coeff. of linear therm. expansion, parallel 150 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm -
Yellow Card available yes - -
Oxygen index 17.5 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4 - IEC 62631-2-1
Relative permittivity, 1MHz 2.9 - IEC 62631-2-1
Dissipation factor, 100Hz 400 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 400 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity 1E13 Ohm IEC 62631-3-2
Comparative tracking index 600 - IEC 60112
Optical propertiesValueUnitTest Standard
ISO Data
Luminous transmittance 89 % ISO 13468-1, -2
Other propertiesValueUnitTest Standard
Water absorption 1.2 % Sim. to ISO 62
Humidity absorption 0.4 % Sim. to ISO 62
Density 1120 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 265 °C ISO 294
Injection Molding, mold temperature 40 °C ISO 294
Injection Molding, injection velocity 195 mm/s ISO 294
Diagrams
Viscosity-shear rate , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
Shearstress-shear rate , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
Dynamic Shear modulus-temperature , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
Stress-strain , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
Secant modulus-strain , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
Stress-strain (isochronous) 23°C, PLEXIGLAS® Resist zk50, PMMA-I, Röhm
Creep modulus-time 23°C, PLEXIGLAS® Resist zk50, PMMA-I, Röhm
Creep curve 23°C, PLEXIGLAS® Resist zk50, PMMA-I, Röhm
Tensile modulus-temperature , PLEXIGLAS® Resist zk50, PMMA-I, Röhm
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Sheet Extrusion, Other Extrusion
Delivery form
Pellets
Additives
Release agent
Special Characteristics
High impact or impact modified, Light stabilized or stable to light, U.V. stabilized or stable to weather, Transparent
Features
Amorphous
Chemical Resistance
Environmental Stress Crack Resistance
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING
Predrying temperature: max. 70 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 230 - 240°C
Mold temperature:50 - 70°C
Profile extrusion
PREPROCESSING
Predrying temperature: max. 70 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 230 - 240 °C
Die temperature: 230 - 240 °C
Sheet extrusion
PREPROCESSING
Predrying temperature: max. 70 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 230 - 240 °C
Die temperature: 230 - 240 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.