Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ GX100 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ GX100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastman Tritan™ GX100 copolyester is a clear plastic that is increasingly popular for protective barriers used to limit the spread of viruses like COVID-19, including sneeze guards where durability and resistance to harsh disinfectants is crucial. Tritan GX100 is a good alternative to polycarbonate (PC) and acrylic (PMMA) for heavy gauge sheet.

Tritan GX100 can be found in a variety of heavy-gauge sheet end uses, including sneeze guards, separation barriers, outdoor signs, displays/in-store fixtures and heat-sensitive applications in hospitals, office buildings, schools, and retailers. It has glasslike clarity and is free of materials of concern, including BPA.

Hospitals prefer Tritan due to its resistance to harsh disinfectants, including Super Sani-Cloth® wipes, Virex®, and a variety of other common hospital cleaning agents. This allows Tritan to resist breakage and discoloration, therefore lasting longer than other alternatives.

Tritan GX100 is also the material of choice for outdoor signs and other end uses that require high durability and heat resistance.

机械性能价值单位Test Standard
ASTM数据
屈服应力 45 MPa ASTM D 638
断裂拉伸强度 46 MPa ASTM D 638
屈服伸长率 7 % ASTM D 638
断裂伸长率 133 % ASTM D 638
弯曲模量 1483 MPa ASTM D 790
洛克硬度 R 114 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 1010 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 133 J/m ASTM D 256
温度 -30 °C -
Izod冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 99.2 °C ASTM D 648
DTUL @ 264 psi 90.9 °C ASTM D 648
维卡温度 110 °C ASTM D 1525
其它性能价值单位Test Standard
吸水率, 24小时 0.18 % ASTM D 570
密度 1180 kg/m³ ASTM D 792
典型数据
加工方法
片材挤出成型, 热成型
特殊性能
经热稳处理的/耐热的, 透明.
特征
防护性能, 热稳定性, 共聚物
应用
汽车, 建材, 电子电气
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.