Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ GX100 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ GX100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Eastman Tritan™ GX100 copolyester is a clear plastic that is increasingly popular for protective barriers used to limit the spread of viruses like COVID-19, including sneeze guards where durability and resistance to harsh disinfectants is crucial. Tritan GX100 is a good alternative to polycarbonate (PC) and acrylic (PMMA) for heavy gauge sheet.

Tritan GX100 can be found in a variety of heavy-gauge sheet end uses, including sneeze guards, separation barriers, outdoor signs, displays/in-store fixtures and heat-sensitive applications in hospitals, office buildings, schools, and retailers. It has glasslike clarity and is free of materials of concern, including BPA.

Hospitals prefer Tritan due to its resistance to harsh disinfectants, including Super Sani-Cloth® wipes, Virex®, and a variety of other common hospital cleaning agents. This allows Tritan to resist breakage and discoloration, therefore lasting longer than other alternatives.

Tritan GX100 is also the material of choice for outdoor signs and other end uses that require high durability and heat resistance.

Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione di snervamento 45 MPa ASTM D 638
Resistenza alla trazione a rottura 46 MPa ASTM D 638
Allungamento a snervamento 7 % ASTM D 638
Allungamento a rottura 133 % ASTM D 638
Modulo a flessione 1483 MPa ASTM D 790
Durezza Rockwell R 114 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 1010 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 133 J/m ASTM D 256
Temperatura -30 °C -
Resistenza all'urto Izod, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
DTUL a 66 psi 99.2 °C ASTM D 648
DTUL a 264 psi 90.9 °C ASTM D 648
Temp.di rammollimento Vicat 110 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Assorbimento d’acqua, 24hr 0.18 % ASTM D 570
Densità 1180 kg/m³ ASTM D 792
Caratteristiche
Processabilità e Forma di Forni
Estrusione di Lastre/Fogli, Termoformatura
Caratteristiche speciali
Stabilizzato o stabile al calore, Trasparente
Caratteristiche
Proprietà di barriera, Stabilità termica, Copolimero
Applicazioni
Automotive, Costruzione, Elettrotecnica ed electrici
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.