Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 100P NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 100P NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.


Delrin® 100P is a high viscosity acetal homopolymer for use in easy-to-fill molds. Delrin® 100P provides a great combination of toughness and strength, improved processing thermal stability and productivity for injection molding, and low VOC emissions.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 2.1 cm³/10min ISO 1133
温度 190 °C -
载荷 2.16 kg -
模塑收缩率, 平行 2.2 % ISO 294-4, 2577
模塑收缩率, 垂直 1.9 % ISO 294-4, 2577
ASTM数据
熔融指数, MFI 1 g/10min ASTM D 1238
温度 190 °C -
负载 2.16 kg -
模压收缩率, 平行 0.0195 mm/mm ASTM D 955
模压收缩率, TD 0.018 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
拉伸模量 2900 MPa ISO 527
屈服应力 70 MPa ISO 527
屈服伸长率 26 % ISO 527
名义断裂伸长率 45 % ISO 527
拉伸蠕变模量, 1h 2700 MPa ISO 899-1
拉伸蠕变模量, 1000h 1500 MPa ISO 899-1
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 400 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 14 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 13 kJ/m² ISO 179/1eA
ASTM数据
拉伸模量 2940 MPa ASTM D 638
拉伸强度 67 MPa ASTM D 638
屈服应力 67 MPa ASTM D 638
屈服伸长率 23 % ASTM D 638
断裂伸长率 80 % ASTM D 638
弯曲模量 2790 MPa ASTM D 790
洛克硬度 R 120 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 120 J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 178 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 95 °C ISO 75-1/-2
热变形温度, 0.45 MPa 155 °C ISO 75-1/-2
维卡软化温度, B 160 °C ISO 306
线性热膨胀系数, 平行 110 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 110 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
Yellow Card 现存 是的 - -
ASTM数据
UL94 燃烧性 HB - UL 94
测试厚度 1.5 mm -
热释放速率, 平行 110 E-6/K ASTM D 696
热释放速率, 垂直 110 E-6/K ASTM D 696
DTUL @ 66 psi 163 °C ASTM D 648
DTUL @ 264 psi 95 °C ASTM D 648
熔点 178 °C ASTM D 3418
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 3.9 - IEC 62631-2-1
相对介电常数., 1MHz 3.9 - IEC 62631-2-1
介质损耗因子, 100Hz 35 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 55 E-4 IEC 62631-2-1
体积电阻率 1E12 Ohm*m IEC 62631-3-1
表面电阻率 2E13 Ohm IEC 62631-3-2
介电强度 41 kV/mm IEC 60243-1
相对漏电起痕指数 600 - IEC 60112
ASTM数据
电介质强度, 短时 16.9 kV/mm ASTM D 149
耗散因素, 1 MHz 0.005 - ASTM D 150
电介质常数, 1 MHz 3.7 - ASTM D 150
表面电阻率 2E14 Ohm ASTM D 257
体积电阻率 4E14 Ohm*cm ASTM D 257
其它性能价值单位Test Standard
吸水性 1.4 % 类似ISO 62
吸湿性 0.3 % 类似ISO 62
密度 1420 kg/m³ ISO 1183
吸水率, 24小时 0.4 % ASTM D 570
吸水率, 平衡 0.28 % ASTM D 570
密度 1420 kg/m³ ASTM D 792
函数
粘度-剪切速度 , Delrin® 100P NC010, POM, DuPont
剪切应力-剪切速度 , Delrin® 100P NC010, POM, DuPont
动态剪切模量-温度 , Delrin® 100P NC010, POM, DuPont
应力-应变.  , Delrin® 100P NC010, POM, DuPont
正割模量-应变.  , Delrin® 100P NC010, POM, DuPont
比容-温度(pvT) , Delrin® 100P NC010, POM, DuPont
拉伸模量-温度 , Delrin® 100P NC010, POM, DuPont
典型数据
加工方法
注塑, 薄膜挤出成型, 管材挤出, 异型材挤出成型, 片材挤出成型, 电线挤出, 其它挤出成型
供货形式
粒料, 自然色
添加剂
润滑剂, 脱模助剂
特征
低排放, 热稳定性, 可焊的, 均聚物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.