Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 100P NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 100P NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.


Delrin® 100P is a high viscosity acetal homopolymer for use in easy-to-fill molds. Delrin® 100P provides a great combination of toughness and strength, improved processing thermal stability and productivity for injection molding, and low VOC emissions.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 2.1 cm³/10min ISO 1133
温度 190 °C -
荷重 2.16 kg -
成形収縮率, 平行 2.2 % ISO 294-4, 2577
成形収縮率, 直角 1.9 % ISO 294-4, 2577
ASTM数据
メルトフローレイト, MFI 1 g/10min ASTM D 1238
温度 190 °C -
荷重 2.16 kg -
成形収縮率., 平行 0.0195 mm/mm ASTM D 955
成形収縮率, 直角 0.018 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 2900 MPa ISO 527
降伏応力 70 MPa ISO 527
降伏ひずみ 26 % ISO 527
破壊呼びひずみ 45 % ISO 527
引張クリープ弾性率, 1h 2700 MPa ISO 899-1
引張クリープ弾性率, 1000h 1500 MPa ISO 899-1
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 400 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 14 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 13 kJ/m² ISO 179/1eA
ASTM数据
引張弾性率 2940 MPa ASTM D 638
引張強度 67 MPa ASTM D 638
降伏応力 67 MPa ASTM D 638
降伏点伸び 23 % ASTM D 638
破断伸び 80 % ASTM D 638
曲げ弾性率 2790 MPa ASTM D 790
ロックウェル硬度 R 120 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 120 J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 178 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 95 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 155 °C ISO 75-1/-2
ビカット軟化温度, B 160 °C ISO 306
線膨張係数, 平行 110 E-6/K ISO 11359-1/-2
線膨張係数, 直角 110 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
Yellow Card 可用 はい - -
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 0.8 mm -
Yellow Card 可用 はい - -
ASTM数据
UL94 燃焼性 HB - UL 94
追加試験片の厚さ 1.5 mm -
線膨張係数, 平行 110 E-6/K ASTM D 696
線膨張係数, 直角 110 E-6/K ASTM D 696
DTUL @ 66 psi 163 °C ASTM D 648
DTUL @ 264 psi 95 °C ASTM D 648
溶融温度 178 °C ASTM D 3418
電気的特性.単位テスト基準
ISO データ
比誘電率, 100Hz 3.9 - IEC 62631-2-1
比誘電率, 1MHz 3.9 - IEC 62631-2-1
誘電正接, 100Hz 35 E-4 IEC 62631-2-1
誘電正接, 1MHz 55 E-4 IEC 62631-2-1
体積抵抗率 1E12 Ohm*m IEC 62631-3-1
表面抵抗率 2E13 Ohm IEC 62631-3-2
耐電圧 41 kV/mm IEC 60243-1
耐トラッキング性 600 - IEC 60112
ASTM数据
耐電圧, 短い時間 16.9 kV/mm ASTM D 149
誘電正接, 1 MHz 0.005 - ASTM D 150
比誘電率, 1 MHz 3.7 - ASTM D 150
表面抵抗率 2E14 Ohm ASTM D 257
体積抵抗率 4E14 Ohm*cm ASTM D 257
その他の特性.単位テスト基準
吸水率 1.4 % Sim. to ISO 62
吸湿率 0.3 % Sim. to ISO 62
密度 1420 kg/m³ ISO 1183
吸水率, 24hr 0.4 % ASTM D 570
吸水率, 平衡 0.28 % ASTM D 570
密度 1420 kg/m³ ASTM D 792
機能
 粘度せん断速度. , Delrin® 100P NC010, POM, DuPont
 せん断応力-せん断速度. , Delrin® 100P NC010, POM, DuPont
 せん断弾性率-温度. , Delrin® 100P NC010, POM, DuPont
 応力-ひずみ. , Delrin® 100P NC010, POM, DuPont
 割線弾性率−ひずみ. , Delrin® 100P NC010, POM, DuPont
 pvT , Delrin® 100P NC010, POM, DuPont
 引張弾性率-温度. , Delrin® 100P NC010, POM, DuPont
特殊な特性
成形加工法.
射出成形., フィルム押出成形., Pipe/Tube Extrusion, 異形押出成形., シート押出成形., Wire/Cable Extrusion, その他の押出成形.
納入形状.
ペレット., ナチュラルカラー
添加剤.
滑剤., 離型剤.
な特性
Low Emission, Thermal Stability, Weldable, Homopolymer
領域別の利用可能性
その他の情報
村遜速揃
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

耐薬品性
5wt%酢酸 (23゚C)
10wt%クエン酸 (23゚C)
10wt%乳酸 (23゚C)
36wt%塩酸 (23゚C)
40wt%硝酸 (23゚C)
38wt%硫酸 (23゚C)
5wt%硫酸 (23゚C)
40wt%硝酸 (23゚C)
塩基
35wt%水酸化ナトリウム (23゚C)
1wt%水酸化ナトリウム (23゚C)
10wt%水酸化アンモニウム (23゚C)
アルコール
イソプロピルアルコール23℃ (23゚C)
メタノール 23℃ (23゚C)
エタノール 23℃ (23゚C)
炭化水素
ヘキサン (23゚C)
トルエン (23゚C)
イソオクタン (23゚C)
ケトン系溶剤
アセトン (23゚C)
エーテル溶剤
ジエチルエーテル (23゚C)
鉱油
SAE 10W40 マルチグレードモーターオイル (23゚C)
SAE 10W40 マルチグレードモーターオイル (130゚C)
SAE 80/90 ハイポイドギアオイル (130゚C)
絶縁油 (23゚C)
標準燃料
ISO 1817液1 (60゚C)
ISO 1817液2 (60゚C)
ISO 1817液3 60℃ (60゚C)
ISO 1817液4 (60゚C)
標準燃料(ISO 1817液C)アルコールなし (23゚C)
標準燃料(ISO 1817液4)アルコールあり (23゚C)
ディーゼル燃料(ISO 1817液F) (23゚C)
ディーゼル燃料(ISO 1817液F) (90゚C)
ディーゼル燃料(ISO 1817液F) (>90゚C)
食塩水
10wt%塩化ナトリウム (23゚C)
10wt%次亜塩素酸ナトリウム (23゚C)
20wt%炭酸ナトリウム (23゚C)
2wt%炭酸ナトリウム (23゚C)
50wt%ジンクロメート (23゚C)
その他
エチルアセテート (23゚C)
過酸化水素 (23゚C)
DOT No.4ブレーキ液 (130゚C)
50wt%エチレングリコール水溶液 (108゚C)
1wt%ノニルフェノキシ-ポリエチレノキシ-エタノール水... (23゚C)
オレイン酸50%+オリーブオイル50% (23゚C)
水 (23゚C)
純水 (90゚C)
5wt%フェノール溶液 (23゚C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.