加工/物理特性 | 价值 | 单位 | Test Standard |
Other Standards[S] |
熔融指数, MFI |
14 |
g/10min |
ASTM D 3307 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
机械性能 | 价值 | 单位 | Test Standard |
ASTM数据 |
弯曲模量 |
590 |
MPa |
ASTM D 790 |
邵氏硬度D |
55 |
- |
ASTM D 2240 |
Other Standards[S] |
拉伸强度 |
25 |
MPa |
ASTM D 3307 |
断裂伸长率 |
300 |
% |
ASTM D 3307 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
热性能 | 价值 | 单位 | Test Standard |
ASTM数据 |
UL94 燃烧性 |
V-0 |
- |
UL 94 |
氧指数 |
95 |
% |
ASTM D 2863 |
Other Standards[S] |
熔点 |
305 |
°C |
ASTM D 4591 |
最高工作温度, 长期 |
260 |
°C |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
电性能 | 价值 | 单位 | Test Standard |
ASTM数据 |
电介质强度, 短时 |
80 |
kV/mm |
ASTM D 149 |
耗散因素, 1 MHz |
0.0002 |
- |
ASTM D 150 |
电介质常数, 1 MHz |
2.03 |
- |
ASTM D 150 |
体积电阻率 |
1E18 |
Ohm*cm |
ASTM D 257 |
其它性能 | 价值 | 单位 | Test Standard |
吸水率, 24小时 |
0.03 |
% |
ASTM D 570 |
密度 |
2150 |
kg/m³ |
ASTM D 792 |
典型数据
加工方法
注塑, 其它挤出成型, 模压/烧结成型, 模压成型
供货形式
粒料
特殊性能
经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
特征
Good Drawdown, 低烟量, 熔体强度, 热稳定性, Tribologic Grade
耐化学试剂
通用耐化学性, 耐环境应力裂纹性
Certifications
可食品接触的, 10/2011认证, FDA 21 CFR认证
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.