Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TABOREX TA 1154 HD - (PE-HD) - Silon s.r.o.

Material Data Center offers the following functions for TABOREX TA 1154 HD:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Taborex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
TABOREX TA 1154 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a TABOREX Masterbatch containing the crosslinking catalyst a “SIOPLAS-SYSTEM”. Pipes which are produced with the SILON grade TABOREX TA 1154 HD fulfil the requirements of ASTM F876, CSA 137.5, EN ISO 15875, BS 7291 and all related standards.
This system allows the compound to be extruded as a normal thermoplastic polymer
and will attain a high level of crosslinking in the processed form. The final product provides all the superior properties associated with crosslinked polyethylene.
Crosslinking Cure
The following methods are recommended:
• Autoclave using saturated steam at 100–115 °C (optimal methode)
• By immersion in hot water at 80–95 °C
• Exposure to low pressure steam
The period required to obtain the final gel content depends on the wall thickness and
the temperature. The exposure times are in the range of 4–8 hours.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 1.8 g/10min ISO 1133
温度 190 °C -
负载 5 kg -
机械性能价值单位Test Standard
ISO数据
断裂应力 24 MPa ISO 527
断裂伸长率 490 % ISO 527
其它性能价值单位Test Standard
密度 948 kg/m³ ISO 1183
Bulk density 520 kg/m³ -
加工推荐(挤出)价值单位Test Standard
1区 160 - 170 °C -
2区 170 - 180 °C -
3区 170 - 190 °C -
4区 170 - 190 °C -
喷嘴温度 190 - 220 °C -
典型数据
加工方法
管材挤出
特征
可交联的, 热稳定性
Certifications
可食品接触的, 可水接触的
应用
建材
地区供应
欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com