Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Sarlink® 3150 - TPV - Teknor Apex Co.

Material Data Center offers the following functions for Sarlink® 3150:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sarlink datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

SARLINK TPV 3100 series are engineered materials designed primarily for general purpose, automotive and industrial applications requiring a good balance of thermal, mechanical, and physical properties. SARLINK 3150, available in NAT and BLK, is a medium hardness, low density, multi-purpose thermoplastic vulcanizate that can be processed by injection molding, blow molding or extrusion for applications such as grips, seals, gaskets, profiles, hose & tubes, bellows, and other articles.



PropertyValueUnitStandard
Tensile properties (Cross Flow Direction)

ISO 37
   Tensile strength at break    5,1 MPa
   Modulus at 100% elongation    1,9 MPa
   Elongation at break   600 %
Hot air aging (168h/150°C, Cross Flow Direction)

ISO 188
   Change in hardness     2 points
   Change in tensile strength at break     7 %
   Change in modulus at 100% elongation     5 %
   Change in elongation at break     8 %
Hot air aging (1000h/135°C, Cross Flow Direction)

ISO 188
   Change in hardness     1 points
   Change in tensile strength at break    -6 %
   Change in modulus at 100% elongation     7
%
   Change in elongation at break    -7
%
Volume swell (70h/125°C in IRM 903 oil) 130 % ISO 1817
Apparent shear viscosity @ 206 1/s, 200°C 270 Pa.s ISO 11443 Capillary
机械性能价值单位Test Standard
ISO数据
23°C时恒定应变下的永久变形, 24h 20 % ISO 815
70°C时恒定应变下的永久变形, 24h 32 % ISO 815
肖氏硬度A 56 - ISO 7619-1
Other Standards[S]
100%应变时的应力 3 MPa ISO 37
断裂应力 TPE 4.1 MPa ISO 37
断裂应变. TPE 240 % ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
其它性能价值单位Test Standard
密度 950 kg/m³ ISO 1183
典型数据
加工方法
注塑, 异型材挤出成型, 其它挤出成型, 吹塑
特殊性能
经耐紫外线处理的/耐气候的
特征
好粘附性能
耐化学试剂
通用耐化学性
应用
汽车, 通用
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.