Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® Vestolen A RELY 5922R 10000 Black - (PE-HD)-CD25 - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® Vestolen A RELY 5922R 10000 Black:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
材料文字说明
SABIC® Vestolen A RELY 5922R 10000 is a grade which has a high density and a bimodal distribution of the molecular mass.
Due to its resistance against slow crack growth (SCG) the material SABIC® Vestolen A RELY 5922R 10000 is considered as PE100-RC and may be used for no dig applications.
Moreover it may be used for the production of thick walled (large diameter and low SDR) pipes for infrastructure and industrial application due to its low sagging characteristics and it shows favorable processing behavior.
This material meets (inter)national standards for use in gas, drinking water and waste water piping.MRS class ISO 12162 MPa = 10.0 (PE 100).
This product is not intended for and must not be used in any pharmaceutical/medical applications.
机械性能 | 价值 | 单位 | Test Standard |
ISO数据 |
拉伸模量 |
1100 |
MPa |
ISO 527 |
屈服应力 |
24 |
MPa |
ISO 527 |
屈服伸长率 |
9 |
% |
ISO 527 |
简支梁缺口冲击强度, +23°C |
26 |
kJ/m² |
ISO 179/1eA |
简支梁缺口冲击强度, -30°C |
10 |
kJ/m² |
ISO 179/1eA |
肖氏硬度D |
62 |
- |
ISO 7619-1 |
热性能 | 价值 | 单位 | Test Standard |
ISO数据 |
热变形温度, 1.80 MPa |
45 |
°C |
ISO 75-1/-2 |
热变形温度, 0.45 MPa |
72 |
°C |
ISO 75-1/-2 |
维卡软化温度, B |
72 |
°C |
ISO 306 |
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.