Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LLDPE R40039EE - (PE-LLD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LLDPE R40039EE:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
SABIC® LLDPE R40039EE is a medium density polyethylene (MDPE) copolymer. It is used for its good stress crack resistance, rigidity, gloss and low warpage. The resin contains UV-stabilizer. It is recommended that SABIC® LLDPE R40039E is grinded before use in rotational moulding applications. Typical applications. Because of the good processing performance and physical properties, SABIC® LLDPE R40039EE is used for the rotational moulding of large industrial and agricultural tanks, trash containers and chemical shipping drums. Due to the good mechanical properties and low warpage this product is typically used for injection moulding of screw closures, caps and housewares. The UV-stabilization provides good protection for the final product. Processing conditions. Moulding cycles vary with mould composition and mould wall thickness, oven temperature and wall thickness of the part being produced. Venting of the mould is recommended. Normal cooling is satisfactory for SABIC®LLDPE R40039EE. Oven temperature °F (°C) = 600 (315). Typical processing temperature for injection moulding machines: 210 - 240 °C. Mechanical properties. Test specimens are prepared from compression moulded sheet made according to ASTM D-1928, procedure C. This product is not intended for and must not be used in any pharmaceutical/medical applications.
机械性能价值单位Test Standard
ISO数据
肖氏硬度D 69 - ISO 7619-1
ASTM数据
屈服应力 18 MPa ASTM D 638
断裂拉伸强度 19 MPa ASTM D 638
断裂伸长率 500 % ASTM D 638
热性能价值单位Test Standard
ASTM数据
维卡温度 117 °C ASTM D 1525
典型数据
加工方法
注塑
特征
共聚物
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.