Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LDPE 2501N0 - (PE-LD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LDPE 2501N0:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
SABIC® LDPE 2501N0 is a grade without additives with a low gel level, which combines good draw down ability with fair optical properties and stiffness. Application SABIC® LDPE 2501N0 is typically used in diaper film, surface protection film, lamination film and in applications where low blocking behavior is required and the presence of slip and anti block is unwanted. Film properties Film properties have been measured at film of 50 ?m with a BUR of 3. The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.
热性能价值单位Test Standard
ISO数据
维卡软化温度, A 98 °C ISO 306
光学特性价值单位Test Standard
ASTM数据
雾度 10 % ASTM D 1003
机械性能(薄膜)价值单位Test Standard
ISO数据
拉伸模量, 平行 150 MPa ISO 527-3
屈服应力, 平行 10 MPa ISO 527-3
继续撕裂强度, 平行 45 N/mm ISO 6383-1
继续撕裂强度, 垂直 45 N/mm ISO 6383-1
ASTM Data
拉伸模量, 垂直 200 MPa ASTM D 882
屈服应力, 垂直 12 MPa ASTM D 882
断裂拉伸强度, 平行 25 MPa ASTM D 882
断裂拉伸强度, 垂直 20 MPa ASTM D 882
断裂伸长率, 平行 200 % ASTM D 882
断裂伸长率, 垂直 500 % ASTM D 882
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com