Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Monprene® RG-10140 - TPE - Teknor Apex Co.

Material Data Center offers the following functions for Monprene® RG-10140:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Monprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Preliminary Data

The Monprene RG-10100 series is a group of high performance thermoplastic elastomers specifically designed for regulated applications including food contact, toys, and children's products. Monprene RG-10140 is a low density, low hardness grade that complies with various US FDA and European regulations and directives for food contact and toy safety and is suitable for injection molding.

Adheres to PP

PropertyValueUnitStandard
Tensile Stress at 100% (across flow)0.569MPaISO 37
Tensile Stress at break (across flow)5MPaISO 37
Tensile Strain at Break (across flow860%ISO 37
Tear Strength (across flow)8.3kN/mISO 34-1
Apparent Viscosity (200 °C, 206 1/s)214PasASTM D3835
加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 8 g/10min ASTM D 1238
温度 200 °C -
负载 5 kg -
机械性能价值单位Test Standard
ISO数据
70°C时恒定应变下的永久变形, 24h 23 % ISO 815
撕裂强度 14 kN/m ISO 34-1
肖氏硬度A 40 - ISO 7619-1
其它性能价值单位Test Standard
密度 888 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 65 °C -
预干燥-时间 2 - 4 h -
注塑熔体温度 182 - 227 °C -
模具温度 27 - 49 °C -
1区 160 - 177 °C -
2区 182 - 204 °C -
3区 193 - 216 °C -
喷嘴温度 182 - 227 °C -
螺杆转速 50 - 100 rpm -
背压 0.172 - 0.689 MPa -
典型数据
加工方法
注塑
供货形式
粒料
添加剂
润滑剂
特殊性能
Translucent
特征
好粘附性能
Certifications
可食品接触的, FDA 21 CFR认证
应用
包装
地区供应
北美, 欧洲, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.