Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of LUVOCOM 3F PAHT CF 9742 BK - PA*-CF - LEHVOSS Group
Material Data Center offers the following functions for LUVOCOM 3F PAHT CF 9742 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Luvocom datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
加工/物理特性 | 价值 | 单位 | Test Standard |
Other Standards[S] |
模塑收缩率, 平行 |
0.1 |
% |
DIN 16901 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
机械性能 | 价值 | 单位 | Test Standard |
ISO数据 |
拉伸模量 |
15000 |
MPa |
ISO 527 |
拉伸强度 |
170 |
MPa |
ISO 527 |
简支梁冲击强度, +23°C |
47 |
kJ/m² |
ISO 179/1eU |
热性能 | 价值 | 单位 | Test Standard |
ISO数据 |
热变形温度, 1.80 MPa |
240 |
°C |
ISO 75-1/-2 |
Other Standards[S] |
线性热膨胀系数, 平行 |
4 |
E-6/K |
DIN 53752 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
电性能 | 价值 | 单位 | Test Standard |
ISO数据 |
表面电阻率 |
100 |
Ohm |
IEC 62631-3-2 |
其它性能 | 价值 | 单位 | Test Standard |
密度 |
1400 |
kg/m³ |
ISO 1183 |
加工推荐(挤出) | 价值 | 单位 | Test Standard |
预干燥-温度 |
130 |
°C |
- |
预干燥-时间 |
6 - 8 |
h |
- |
注塑熔体温度 |
280 |
°C |
- |
1区 |
260 - 300 |
°C |
- |
2区 |
260 - 300 |
°C |
- |
3区 |
260 - 300 |
°C |
- |
喷嘴温度 |
250 - 290 |
°C |
- |
典型数据
加工方法
其它挤出成型, Additive Manufacturing
供货形式
粒料, 黑色, 自然色
特殊性能
经热稳处理的/耐热的
应用
汽车, Filament for 3D Printing
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.