Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kepstan® 6002 - PAEK - ARKEMA

Material Data Center offers the following functions for Kepstan® 6002:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kepstan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
KEPSTAN® PEKK resin is a high performance thermoplastic material, based on PolyEtherKetoneKetone (PEKK) highly stable chemical backbone. KEPSTAN® PEKK is a unique member of the PAEK family that incorporates distinctive structural features that allow for exceptional possibilities in the control of crystallinity. These features include a low Ether/Ketone ratio and a copolymer structure incorporating Terephtalic and Isophtalic moieties.

The 6000 Series represents the pseudo-amorphous products of the KEPSTAN® family, offering the lowest melting point and the slowest crystallization behavior, while keeping Tg close to 160°C. These properties allow for lower processing temperatures (as low as 320-330°C), and lead to glassy or semi crystalline structures, depending on processing technologies and cooling conditions.

KEPSTAN® 6000 Series includes a medium flow grade, KEPSTAN® 6002, and a high flow grade, KEPSTAN® 6003, both unfilled PEKK resins designed to meet the requirements of a broad range of processing technologies, including among others extrusion, calendering, thermoforming, injection molding, fiber impregnation, rotomolding, powder coating, bonding and welding. 

KEPSTAN® PEKK resin is available in pellet form as well as in powder form with different particle sizes. Standard packaging includes 20 kg boxes for pellets and 10 kg boxes for powders.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 35 cm³/10min ISO 1133
温度 380 °C -
载荷 5 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2900 MPa ISO 527
屈服应力 88 MPa ISO 527
屈服伸长率 5.4 % ISO 527
断裂伸长率 >50 % ISO 527
弯曲模量, 23°C 3000 MPa ISO 178
简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 5.5 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 5 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 302 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 160 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 139 °C ISO 75-1/-2
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
燃烧性-氧指数 38 % ISO 4589-1/-2
电性能价值单位Test Standard
ISO数据
相对介电常数., 1MHz 3 - IEC 62631-2-1
介电强度 84 kV/mm IEC 60243-1
ASTM数据
表面电阻率 >1E15 Ohm ASTM D 257
体积电阻率 >1E15 Ohm*cm ASTM D 257
其它性能价值单位Test Standard
吸水性 1.07 % 类似ISO 62
吸湿性 0.44 % 类似ISO 62
密度 1270 kg/m³ ISO 1183
典型数据
加工方法
注塑, 纤维挤出, 异型材挤出成型, 片材挤出成型, 其它挤出成型, 表面涂层, 吹塑, 压延成型, 模压/烧结成型, 热成型, 旋转成型
供货形式
粒料, 粉料
特征
无定形
地区供应
其他信息
注塑成型
Drying temperature and time: 120°C for 6 to 8 hours
Processing temperature: 320 – 360°C
Temperature settings - Injection: Rear 300°C / Center 315°C / Front 320°C / Nozzle 330°C
Mold temperature (below Tg in any case): 80 - 120°C
Temperature settings - Extrusion:  Zones 1/2/3/4: 290°C/ 320°C/ 330°C/ 320°C   Die: 320°C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com