Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Hifax - PP - LyondellBasell Industries

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Hifax" in Material Data Center leads to the following information:

Tradename: Hifax
Family: PP
Producer: LyondellBasell Industries
301 hits in the material database
2 hits in the literature database
1 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Friction Behaviour of Thermoplastics
...aratus is mounted. Design of the Test Apparatus The plastic test specimens used were injection moulded plaques. Polycarbonate, PC (grade: Lexan 141R, manufacturer: GE Plastics) was used to represent amorphous plastics and polypropylene, PP (grade: Hifax BA238B3, manufacturer: Montell) for semi-crystalline. The steel stamps used have finely machined, flat, ground surfaces measuring 10 x 60 mm with different surface roughness values and machined in various directions (Table 1). In the test appar...

Kunststoffe international, 2010-09-24, Raising the Standards
...product changes and higher turnovers. Hostalen CRP 100 Resit CR black, an PE-HD pipe material, is being produced using the ACP technology, enabling customer demands to higher cracking resistance to be satisfied. In the automotive sector, a Hifax PP is replacing the conventional ABS in bumper elements, i.a. in the BMW X1 (Fig. 4). The PP compound with aluminum flake pigment creates a metallic effect and makes subsequent painting of the component superfluous. With the same result, savings are also...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.