Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grilon BS natural - PA6 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grilon BS natural:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Grilon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Product-nomenclature: ISO 16396-PA6,,M1HR,S14-030N

 

Product Attributes

  Nucleated

Markets

  Automotive
  Powertrain and Chassis, Interior
  Electricals & Electronics
  Electrical appliances, Electrical equipment
  Industry & Consumer goods
  Housewares, Mechanical Engineering, Sports & Leisure, Tools & Accessories
加工/物理特性干 / 已调节单位Test Standard
ISO数据
模塑收缩率, 平行 1.0 / * % ISO 294-4, 2577
模塑收缩率, 垂直 1.3 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 3000 / 1000 MPa ISO 527
屈服应力 80 / 40 MPa ISO 527
屈服伸长率 4 / 15 % ISO 527
名义断裂伸长率 15 / >50 % ISO 527
无缺口简支梁冲击强度, +23°C N / N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N / N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 5 / 30 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 5 / 4 kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 222 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 60 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 175 / * °C ISO 75-1/-2
线性热膨胀系数, 平行 80 / * E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 80 / * E-6/K ISO 11359-1/-2
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 0.8 / * mm -
电性能干 / 已调节单位Test Standard
ISO数据
体积电阻率 1E11 / 1E9 Ohm*m IEC 62631-3-1
表面电阻率 * / 1E11 Ohm IEC 62631-3-2
介电强度 30 / 27 kV/mm IEC 60243-1
相对漏电起痕指数 - / 600 - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 9 / * % 类似ISO 62
吸湿性 3 / * % 类似ISO 62
密度 1130 / - kg/m³ ISO 1183
函数
粘度-剪切速度 , Grilon BS natural, PA6, EMS-GRIVORY
剪切应力-剪切速度 , Grilon BS natural, PA6, EMS-GRIVORY
动态剪切模量-温度 , Grilon BS natural (烘干), PA6, EMS-GRIVORY
动态剪切模量-温度 , Grilon BS natural (状况), PA6, EMS-GRIVORY
应力-应变.  , Grilon BS natural (烘干), PA6, EMS-GRIVORY
应力-应变.  , Grilon BS natural (状况), PA6, EMS-GRIVORY
正割模量-应变.  , Grilon BS natural (烘干), PA6, EMS-GRIVORY
正割模量-应变.  , Grilon BS natural (状况), PA6, EMS-GRIVORY
比容-温度(pvT) , Grilon BS natural, PA6, EMS-GRIVORY
拉伸模量-温度 , Grilon BS natural (烘干), PA6, EMS-GRIVORY
典型数据
加工方法
注塑
供货形式
碎粒料, 自然色
添加剂
润滑剂
特征
有核的
应用
汽车, 电子电气, 运动器械
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.