Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Genestar™ G1352A-M41 - PA9T-GF35 - Kuraray Co., Ltd.

Material Data Center offers the following functions for Genestar™ G1352A-M41:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Genestar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

GENESTAR G1352A-M41 is a 35% GF reinforced injection molding grade with improved tribological properties. 


The mean features are:

  • Performance at high temperature
  • Low wear and friction
  • Dimensional stability

This grade is suitable for reinforced friction applications.


加工/物理特性价值单位Test Standard
ISO数据
模塑收缩率, 平行 0.2 % ISO 294-4, 2577
模塑收缩率, 垂直 0.8 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 11600 MPa ISO 527
断裂应力 200 MPa ISO 527
断裂伸长率 2.5 % ISO 527
简支梁缺口冲击强度, +23°C 13 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 300 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 125 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 270 °C ISO 75-1/-2
ASTM数据
热释放速率, 平行 17 E-6/K ASTM D 696
热释放速率, 垂直 45 E-6/K ASTM D 696
其它性能价值单位Test Standard
吸水性 0.14 % 类似ISO 62
密度 1500 kg/m³ ISO 1183
函数
应力-应变.  , Genestar™ G1352A-M41, PA9T-GF35, Kuraray
正割模量-应变.  , Genestar™ G1352A-M41, PA9T-GF35, Kuraray
比容-温度(pvT) , Genestar™ G1352A-M41, PA9T-GF35, Kuraray
典型数据
加工方法
注塑
供货形式
黑色
添加剂
润滑剂, 脱模助剂
特殊性能
经热稳处理的/耐热的
特征
防护性能, 防蠕变, 防老, 高结晶度, 热稳定性, Tribologic Grade, 可焊的
耐化学试剂
耐酸性, 耐碱性, 通用耐化学性, 耐环境应力裂纹性, 耐溶剂性, 耐油脂性, 水解稳定, 耐油性
应用
汽车, 通用
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.