Material datasheets available free. Online registration at: www.materialdatacenter.com
Europrene - BR, NBR, TPR - Versalis S.p.A
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Europrene" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...upling agent, further improve the roll resistance and especially the abrasion resistance of tyres through the changed macrostructure. In addition to the MES (morpholino ethane sulphonic acid)-stretched Europrene SOL R 72612 (25% bound styrene, vinyl content 67%), Polimeri Europa, Ravenna, Italy manufactures a new aromatic-free, oil-stretched S-SBR grade (vinyl content 64%) based on labelling-free tetrakis dimethyl amino ethylene (TDAE). Similar safe-oil-stretched grades are also available in E-S...
Kunststoffe international, 2005-11-21, Elastomers
...BR), in order to meet growing demand for modern tyre-tread blends. For example, in the past five years, Bayer doubled capacities for SBR and BR to 550kt/a. EniChem/Polimeri Europa, with Europrene SOLR72612 offers a new S-SBR grade for silica-filled compounds. Similar grades are offered by Zeon with NipolNS112R and 116R. Zeon is also continuing to develop its E-SBR range in order to match the high mechanical level and outstanding processability of S-SBR. Dow is now offering Co, Li and Ni catalyse...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.