Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 100T NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 100T NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 100T is a toughened, high viscosity acetal homopolymer with superior impact resistance.  It is designed for highly stressed parts where outstanding toughness is required.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 1.9 cm³/10min ISO 1133
温度 190 °C -
载荷 2.16 kg -
模塑收缩率, 平行 1.3 % ISO 294-4, 2577
模塑收缩率, 垂直 1.5 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 1900 MPa ISO 527
屈服应力 55 MPa ISO 527
屈服伸长率 25 % ISO 527
名义断裂伸长率 >50 % ISO 527
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 26 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 14 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 178 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 72 °C ISO 75-1/-2
热变形温度, 0.45 MPa 130 °C ISO 75-1/-2
线性热膨胀系数, 平行 120 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 120 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
电性能价值单位Test Standard
ISO数据
介质损耗因子, 1MHz 90 E-4 IEC 62631-2-1
体积电阻率 6E12 Ohm*m IEC 62631-3-1
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
吸水性 0.9 % 类似ISO 62
吸湿性 0.3 % 类似ISO 62
密度 1370 kg/m³ ISO 1183
函数
粘度-剪切速度 , Delrin® 100T NC010, POM, DuPont
剪切应力-剪切速度 , Delrin® 100T NC010, POM, DuPont
动态剪切模量-温度 , Delrin® 100T NC010, POM, DuPont
应力-应变.  , Delrin® 100T NC010, POM, DuPont
正割模量-应变.  , Delrin® 100T NC010, POM, DuPont
比容-温度(pvT) , Delrin® 100T NC010, POM, DuPont
典型数据
加工方法
注塑, 异型材挤出成型, 片材挤出成型, 其它挤出成型
供货形式
粒料, 自然色
添加剂
润滑剂, 脱模助剂
特殊性能
高冲击韧性的/经抗冲改性的
特征
均聚物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.