Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LLDPE 6335BE - (PE-LLD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LLDPE 6335BE:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
SABIC® LLDPE 6335BE is a hexene linear low density polyethylene resin for cast film applications. The product has been specially formulated for optimum thermal stability at high temperatures used in cast film extrusion. Cast films produced from SABIC® LLDPE 6335BE exhibit excellent optical properties, toughness, puncture resistance, tear strength and stiffness. Application SABIC® LLDPE 6335BE resin is recommended for use in non cling layers in pallet stretch wrap (pre-stretch), high performance draw down films and other mono layer and coextruded film applications where high strength is required. Film properties Properties are determined on 20 ?m cast stretch film produced on a 2 m commercial cast stretch film line: melt temperature 270 °C, chill roll temperature 20 °C and line speed 450 m/min. Processing conditions SABIC® LLDPE 6335BE is extrudable with conventional cast film extrusion equipment. Minor machine modification may be required for optimum use. Cast film melt temperatures 250 - 300 °C. The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications.
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Температура размягчения по Вика, A 117 °C ISO 306
Оптические свойстваЗначениеЕдиницаСтандарт
Данные ASTM
Мутность 3.1 % ASTM D 1003
Свойства пленкиЗначениеЕдиницаСтандарт
Данные ISO
Сопротивление распространению раздира, поперечное 227 Н/мм ISO 6383-1
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.