Adflex - PP - LyondellBasell Industries
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Adflex" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...ftest grade, Softell Q20F, exhibits an elastic modulus of 20 MPa and a hardness of 75 Shore A, which corresponds to that of flexible PVC. Transparency, however, is apparently no longer a possibility in terms of further development of the Adflex line. Modification takes place after the reactor – and new modifiers are opening up new possibilities here. New in this regard are the ethylene/propene elastomers, specifically the products Versify (Dow) [4] and Vistamaxx (Exxon), while elastomers based o...
Kunststoffe international, 2011-10-17, Polypropylene (PP)
...d SC820CF, a soft heterophasic copolymer with random EP matrix, has been developed specifically for medical infusion bags and packaging for medical instruments (Fig. 4). Although it does not quite match the extreme softness of LyondellBasell Adflex grades, the focus is on striking the right balance of flexibility, transparency and ease of sterilization. Generally, polyolefins are also benefiting in this regard from the debate concerning adverse effects of the plasticizers used in plasticized PVC...
Kunststoffe international, 2014-10-10, Polypropylene (PP)
...hole new developments in the film sector are taking place with extremely flexible grades – an area long exclusively covered by Lyondellbasell Industries AF S.C.A. (LyondellBasell), Rotterdam, Netherlands, with its Adflex grades produced by the Catalloy process in an elastic modulus range from 400 to 100 MPa. Just recently, Borealis launched Bormed SC876CF, the latest development in the area of flexible, transparent polypropylene specially designed for challenging medical packaging. Even in tests...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.