Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PAHT CF15 - PA*-CF15 - BASF

Material Data Center offers the following functions for Ultrafuse PAHT CF15:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 42.2 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 234 / * °C ISO 11357-1/-3
Temp. de transição vítrea, 10 °C/min 70 / * °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 92 / * °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 145 / * °C ISO 75-1/-2
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1230 / 1230 kg/m³ ISO 1183
3D DataSeco / CondUnidadeMétodo de ensaio
Other Standards[S]
Módulo de tração, flat 8390 / 5050 MPa ISO 527
Módulo de tração, upright 3530 / 2460 MPa ISO 527
Resistência à tração, flat 103 / 62.9 MPa ISO 527
Resistência à tração, upright 18.2 / 19.1 MPa ISO 527
Deformação na ruptura, flat 1.8 / 2.9 % ISO 527
Deformação na ruptura, upright 0.5 / 0.8 % ISO 527
Módulo de flexão, flat 8260 / 6060 MPa ISO 178
Módulo de flexão, on-edge 7670 / 6260 MPa ISO 178
Módulo de flexão, upright 2710 / 2190 MPa ISO 178
Resistência à flexão, flat 161 / 125 MPa ISO 178
Resistência à flexão, on-edge 172 / 122 MPa ISO 178
Resistência à flexão, upright 50.8 / 56 MPa ISO 178
Resistência ao impacto Charpy, +23°C, flat 20.6 / 21.9 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, +23°C, on-edge 19.3 / 20.4 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, +23°C, upright 2.9 / 2.8 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C, flat 4.8 / 5.1 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, +23°C, on-edge 3.9 / 5.3 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, +23°C, upright 1.3 / 1.6 kJ/m² ISO 179/1eA
Resistência ao Impacto Izod, +23°C, flat 16.4 / 16.3 kJ/m² ISO 180/1U
Resistência ao Impacto Izod, +23°C, on-edge 18.1 / 15.1 kJ/m² ISO 180/1U
Resistência ao Impacto Izod, +23°C, upright 2.9 / 4.1 kJ/m² ISO 180/1U
Impacto Izod com entalhe, +23°C, flat 4.9 / 6.5 kJ/m² ISO 180/1A
Impacto Izod com entalhe, +23°C, on-edge 5.1 / 5.8 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Características
Processamento
Additive Manufacturing
Forma de entrega
Monofilament
Características especiais
Estável contra o calor
Resistência Química
Resistência química geral
Disponibilidade regional
América do Norte, Europa, America Centra e do Sul
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.