Material datasheets available free. Online registration at: www.materialdatacenter.com
Supradel - PPSU - Solvay Specialty Polymers
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Supradel" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...olyphenylsulphone’s premiere in the Airbus was expedited by its high transparency, notch impact resistance and low environmental stress cracking. With a glass transition temperature of 265°C and a heat deflection temperature of 255°C, Supradel, the polysulphone from Solvay, is more heat resistant than all the transparent, amorphous polymers currently found on the market. In contrast to polyamide, it has higher resistance to moisture and can also be injection moulded. In practice it can be substi...
Kunststoffe international, 2005-11-21, Impressive Variety: Polysulfones (PSU, PESU, PPSU)
...ated market introduction of a next-generation sulfone polymer in which the upper temperature limit in use has been raised even considerably higher. With a glass transition temperature of 265°C, this new high-temperature polymer with the trade name Supradel HTS currently represents the peak performer among amorphous thermoplastics. Focus on Applications The growing interest in the performance potential of sulfone polymers is leading continually to new applications for this interesting group of ...
Kunststoffe international, 2005-11-21, Sulphone Polymers: Clear Vision
.... 1000 cycles). Its typical applications lie in medical and food technology. Unique: Transparent Substitute for Metal At K2004, Solvay Advanced Polymers introduced a totally new transparent high-temperature sulphone polymer with the trade name Supradel HTS. With a glass transition temperature of 265°C and a heat deflection temperature (HDT/A) of 255°C, this new HT plastic offer the highest heat resistance of any amorphous thermoplastic polymer commercially available today. This is manifested in ...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.