Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PP FPC70 - PP - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PP FPC70:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
As part of SABIC® PP FLOWPACT portfolio, FPC70 delivers high top load performance (potential downgauging) with a superior stiffness / impact balance. It is nucleated and has good antistatic performance with easy demoulding. This grade has good flow behavior, and it was designed for high-speed injection moulding process, potentially enabling very cost efficient processing on the basis of easy mould filling and very short cycle times. Applications: SABIC® PP FPC70 is typically used in rigid packaging applications for both food and non-food industries. This includes packaging for yellow fats, cheese spreads, dairy, frozen, chilled and ambient food, household chemicals and paints among others. It can be also used in several applications in the caps & closures as well in housewares. The grade has excellent heat deflection temperature making it particularly suitable for hot fill applications. Health, Safety and Food Contact regulations: Material Safety Data Sheets (MSDS) and Product Safety declarations are available on our Internet site http://www.SABIC.com This product is not intended for and must not be used in any pharmaceutical/medical applications.
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 1700 MPa ISO 527
Tensão no escoamento 28 MPa ISO 527
Deformação no escoamento 4 % ISO 527
Impacto Izod com entalhe, +23°C 6 kJ/m² ISO 180/1A
Impacto Izod com entalhe 4 kJ/m² ISO 180/1A
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 60 °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 100 °C ISO 75-1/-2
Temperatura de amolecimento Vicat , A 150 °C ISO 306
Temperatura de amolecimento Vicat, B 80 °C ISO 306
Características
Certifications
Contacto com alimentos
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.