Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PC Resin PC0800 - Europe - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PC Resin PC0800 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
PC0800 resin is a low flow (MFR = 8 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It is available exclusively at www.sabicpc.com.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 7 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
ASTM Dados
Índice de fluidez, MFI 8 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2350 MPa ISO 527
Tensão no escoamento 63 MPa ISO 527
Deformação no escoamento 6 % ISO 527
Deformação na ruptura 50 % ISO 527
Módulo de flexão 2300 MPa ISO 178
Dureza Rockwell R 120 - ISO 2039-2
ASTM Dados
Módulo de tração 2350 MPa ASTM D 638
Resistência à tração no escoamento 63 MPa ASTM D 638
Alongamento no escoamento 6 % ASTM D 638
Deformação na ruptura 70 % ASTM D 638
Módulo de flexão 2300 MPa ASTM D 790
Dureza Rockwell R 120 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 900 J/m ASTM D 256
Resistência ao Impacto Izod, 1/8 in N J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 127 °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 138 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 144 °C ISO 306
Flamabilidade a 1.5mm esp. nom. V-2 class IEC 60695-11-10
Espessuras do tubo de teste 1.6 mm -
Condutividade térmica 0.2 W/(m K) DIN 52616
ASTM Dados
DTUL @ 66 psi 138 °C ASTM D 648
DTUL @ 264 psi 127 °C ASTM D 648
Temperatura de amolecimento Vicat 144 °C ASTM D 1525
Condutividade térmica, estado sólido 0.0288 W/(m K) ASTM C 177
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 1MHz 3 - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 10 E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 100 E-4 IEC 62631-2-1
Resistividade volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistência elétrica 27 kV/mm IEC 60243-1
ASTM Dados
Resistência elétrica, tempo curto 27 kV/mm ASTM D 149
Fator de dissipação dielétrica, 60 Hz 0.001 - ASTM D 150
Fator de dissipação dielétrica, 1 MHz 0.01 - ASTM D 150
Constante dielétrica, 60 Hz 3 - ASTM D 150
Constante dielétrica, 1 MHz 3 - ASTM D 150
Resistividade volumétrica específica 1E15 Ohm*cm ASTM D 257
Propriedades ópticasValorUnidadeMétodo de ensaio
ASTM Dados
Haze 0.8 % ASTM D 1003
Transmitância luminosa 90 % ASTM D 1003
Índice de refração 1.59 - ASTM D 542
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água 0.35 % Sim. to ISO 62
Densidade 1200 kg/m³ ISO 1183
Absorção de água, equilíbrio 0.35 % ASTM D 570
Densidade 1200 kg/m³ ASTM D 792
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura ≤120 °C -
Pré-secagem - tempo 2 - 4 h -
Temperatura da massa 290 - 320 °C -
Temperatura do molde 80 - 120 °C -
Zona 1 270 - 300 °C -
Zona 2 280 - 310 °C -
Zona 3 290 - 320 °C -
Temperatura do bico 280 - 310 °C -
Características
Características especiais
Estabilidade a raios U.V./Intempéries, Estável contra o calor
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.