Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LDPE 2102N3W - (PE-LD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LDPE 2102N3W:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
SABIC® LDPE 2102N3W is a general purpose grade with a high level of anti block and slip agent. This grade offers good optical properties and a very good draw down ability. Application SABIC® LDPE 2102N3W is typically used for packaging films for food and industrial goods and for lamination films. This grade is typically used when high draw down is required The usual melt-2 film thickness can be reduced by 10-40%, maintaining an adequate CoF level. SABIC® LDPE 2102N3W can typically be used for food applications due to very low migration levels. Film properties Film properties have been measured at film of 25 ?m with a BUR of 3. The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de amolecimento Vicat , A 90 °C ISO 306
Propriedades ópticasValorUnidadeMétodo de ensaio
ASTM Dados
Haze 12 % ASTM D 1003
Propriedades do filmeValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração, perpend. 190 MPa ISO 527-3
Tensão no escoamento, paralelo 13 MPa ISO 527-3
Tensão no escoamento, perpend. 11 MPa ISO 527-3
Tensão na ruptura, paralelo 30 MPa ISO 527-3
Tensão na ruptura, perpend. 18 MPa ISO 527-3
Resistência ao rasgamento Trouser, paralelo 50 N/mm ISO 6383-1
Resistência ao rasgamento Trouser, perpend. 20 N/mm ISO 6383-1
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.