Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Kynar® HSV 1800 - PVDF - ARKEMA
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Kynar datasheets, application examples or technical articles are available in Material Data Center
Kynar® HSV1800 is a commercial functional homopolymer of vinylidene fluoride, specifically designed to be used as a cathode binder in Lithium Ion Batteries.
Main Characteristics:
• Highadhesion
• Excellent cathode slurry stability with Nickel Manganese Cobalt Active Materials
• High molecularweight
• Functional
Main applications:
- Battery
Outras propriedades | Valor | Unidade | Método de ensaio |
Densidade | 1780 | kg/m³ | ISO 1183 |
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.