Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of FIL-A-GEHR ABS® - ABS - Gehr GmbH
Material Data Center offers the following functions for FIL-A-GEHR ABS®:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Fil-A-Gehr datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Informação do produto
To determine the FIL-A-GEHR ABS® data, ISO 527 tensile test speciment were printed with the following parameters: Infill 20%, TPrint 245°C, TBed 110°C, Layer thickness 0,2 mm, Outlines 3, Nozzle diameter 0,5 mm, Wall thickness 1,5 mm, Infill rectilinear, Printing speed 50 mm/s, Multiplier 100, Slicer Simplify3D
Características de processamento/físicas | Valor | Unidade | Método de ensaio |
ISO Dados |
Índice de fluidez volumétrico, MVR |
31[1] |
cm³/10min |
ISO 1133 |
Temperatura |
220 |
°C |
- |
Carga |
10 |
kg |
- |
1: | Data based on raw material |
Propriedades mecânicas | Valor | Unidade | Método de ensaio |
ISO Dados |
Módulo de tração |
2400[2] |
MPa |
ISO 527 |
Tensão no escoamento |
46[2] |
MPa |
ISO 527 |
Res. impacto Charpy c/entalhe, +23°C |
15[2] |
kJ/m² |
ISO 179/1eA |
Impacto Izod com entalhe, +23°C |
15[2] |
kJ/m² |
ISO 180/1A |
Ball indentation hardness |
105[2] |
MPa |
ISO 2039-1 |
2: | Data based on raw material |
Propriedades térmicas | Valor | Unidade | Método de ensaio |
ISO Dados |
Temperatura de fusão, 10°C/min |
245[3] |
°C |
ISO 11357-1/-3 |
Temperatura de deflexão térmica, 1.80 MPa |
94[3] |
°C |
ISO 75-1/-2 |
3: | Data based on raw material |
Outras propriedades | Valor | Unidade | Método de ensaio |
Densidade |
1050[4] |
kg/m³ |
ISO 1183 |
4: | Data based on raw material |
3D Data | Valor | Unidade | Método de ensaio |
Módulo de tração, flat |
1270[5] |
MPa |
- |
Módulo de tração, upright |
1730[5] |
MPa |
- |
Resistência à tração, flat |
23.3[5] |
MPa |
- |
Resistência à tração, upright |
20.5[5] |
MPa |
- |
Características
Processamento
Additive Manufacturing
Forma de entrega
Monofilament
Características especiais
Alto impacto., Estável contra o calor
Características
Boa adesão, Baixo odor
Certifications
Contacto com alimentos
Aplicaciones
Médico
Disponibilidade regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.